Cyclic inelastic behavior and shakedown response of a 2nd generation nickel-base single crystal superalloy under tension-torsion loadings: Experiments and simulations 期刊论文
EUROPEAN JOURNAL OF MECHANICS A-SOLIDS, 2020, 卷号: 80, 页码: 10
Authors:  Zhang, Zhen;  Cinoglu, I. Soner;  Charbal, Ali;  Vermaak, Natasha;  Lou, Langhong;  Zhang, Jian
Favorite  |  View/Download:134/0  |  Submit date:2021/02/02
Shakedown  Inelastic design  Cyclic loading  Elastic-perfectly-plastic  Nickel-base single crystal superalloy  Tension-torsion loadings