Effect of melt superheat treatment on solidification behavior and microstructure of new Ni-Co based superalloy 期刊论文
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2021, 卷号: 15, 页码: 4970-4980
作者:  Cui, Hongyang;  Tan, Yi;  Bai, Rusheng;  Li, Yi;  Zhao, Longhai;  Zhuang, Xinpeng;  Wang, Yilin;  Chen, Ziang;  Li, Pengting;  You, Xiaogang;  Cui, Chuanyong
收藏  |  浏览/下载:124/0  |  提交时间:2022/01/27
Superheat treatment  Dendritic segregation  Microstructure refinement  New Ni-Co Based superalloy  
Effect of Si on the Solidification Segregation Behavior of a New Ni-Co-Based Superalloy 期刊论文
ADVANCED ENGINEERING MATERIALS, 2021, 页码: 11
作者:  Zhuang, Xinpeng;  Tan, Yi;  You, Xiaogang;  Cui, Hongyang;  Cui, Chuanyong;  Zhao, Longhai;  Li, Pengting
收藏  |  浏览/下载:119/0  |  提交时间:2021/10/15
new Ni-Co-based superalloy  segregations  silicon  solidifications  
High temperature oxidation behavior and mechanism of a new Ni-Co-based superalloy 期刊论文
VACUUM, 2021, 卷号: 189, 页码: 9
作者:  Zhuang, Xinpeng;  Tan, Yi;  You, Xiaogang;  Li, Pengting;  Zhao, Longhai;  Cui, Chuanyong;  Zhang, Huixing;  Cui, Hongyang
收藏  |  浏览/下载:127/0  |  提交时间:2021/10/15
Ni-Co-based superalloy  Oxidation behavior  Oxide layer  Oxidation mechanism  
Microstructural evolution of a Ni-Co based superalloy during hot compression at gamma ' sub-/super-solvus temperatures 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 卷号: 77, 页码: 66-81
作者:  Liu, Peng;  Zhang, Rui;  Yuan, Yong;  Cui, Chuanyong;  Liang, Faguang;  Liu, Xi;  Gu, Yuefeng;  Zhou, Yizhou;  Sun, Xiaofeng
收藏  |  浏览/下载:151/0  |  提交时间:2021/10/15
Ni-Co based superalloy  Strain rate  Primary gamma ' precipitates  Dynamic recrystallization  Microstructural evolution  
Microstructural evolution of a Y2O3 network reinforced Ni-Co based superalloy fabricated by spark plasma sintering 期刊论文
VACUUM, 2021, 卷号: 186, 页码: 12
作者:  Bai, Yingbo;  Zhang, Rui;  Qi, Yang;  Cui, Chuanyong;  Cai, Yahui
收藏  |  浏览/下载:149/0  |  提交时间:2021/10/15
Reinforcement network distribution  Spark plasma sintering  Ni-Co based Superalloy  Microstructural evolution  
Effects of Homogenization Treatment on the Microsegregation of a Ni-Co Based Superalloy Produced by Directional Solidification 期刊论文
ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2021, 页码: 12
作者:  Zhou, Zijian;  Zhang, Rui;  Cui, Chuanyong;  Zhou, Yizhou;  Sun, Xiaofeng
收藏  |  浏览/下载:164/0  |  提交时间:2021/03/15
Ni–  Co based superalloy  Element segregation  Homogenization  Diffusion kinetics