IMR OpenIR

Browse/Search Results:  1-8 of 8 Help

Filters    
Selected(0)Clear Items/Page:    Sort:
Effect of Mo Addition on Microstructural Characteristics in a Re-containing Single Crystal Superalloy 期刊论文
Journal of Materials Science & Technology, 2015, 卷号: 31, 期号: 2, 页码: 143-147
Authors:  X. G.;  Wang Liu, L.;  Lou, L. H.;  Zhang, J.
Favorite  |  View/Download:66/0  |  Submit date:2015/05/08
Superalloy  Molybdenum  Microstructure  Partitioning Behavior  Lattice  Misfit  Nickel-base Superalloys  Lattice Mismatch  Creep  Molybdenum  Phases  Misfit  
Effect of Long-term Thermal Exposure on Microstructure and Stress Rupture Properties of GH3535 Superalloy 期刊论文
Journal of Materials Science & Technology, 2015, 卷号: 31, 期号: 3, 页码: 269-279
Authors:  T.;  Dong Liu, J. S.;  Wang, L.;  Li, Z. J.;  Zhou, X. T.;  Lou, L. H.;  Zhang, J.
Favorite  |  View/Download:82/0  |  Submit date:2015/05/08
Gh3535 Superalloy  Long Term Thermal Exposure  Microstructure  Carbide  M6c  M12c  Stress Rupture Properties  Nickel-base Superalloy  Carbide  Evolution  
Thermal Stability of a New Ni-Fe-Cr Base Alloy with Different Ti/Al Ratios 期刊论文
Journal of Materials Science & Technology, 2015, 卷号: 31, 期号: 2, 页码: 135-142
Authors:  C. S.;  Wang Wang, T. T.;  Tan, M. L.;  Guo, Y. G.;  Guo, J. T.;  Zhou, L. Z.
Favorite  |  View/Download:95/0  |  Submit date:2015/05/08
700 Degrees c A-usc  Ni-fe-cr Base Alloy  Thermal Stability  Eta Phase  Ti/al Ratio  Nickel-based Superalloy  Coal Power-plants  Mechanical-properties  Eta-phase  Microstructure  
Anisotropic Creep Rupture Properties of a Nickel-base Single Crystal Superalloy at High Temperature 期刊论文
Journal of Materials Science & Technology, 2011, 卷号: 27, 期号: 2, 页码: 107-112
Authors:  S. H. Zhang;  J. A. Zhang;  L. H. Lou
Adobe PDF(1079Kb)  |  Favorite  |  View/Download:54/0  |  Submit date:2012/04/13
Nickel-base Single Crystal Superalloy  Stress Rupture Property  Orientation  Dislocation  Particle Hardening Mechanisms  Orientation Dependence  Cmsx-4  Deformation  Alloys  Solidification  Freckles  Behavior  
Microstructural stability of a single crystal superalloy DD8 during thermal exposure 期刊论文
Journal of Materials Science & Technology, 2008, 卷号: 24, 期号: 1, 页码: 127-130
Authors:  K. Y. Cheng;  D. H. Kim;  Y. S. Yoo;  C. Y. Jo;  T. Jin;  Z. Q. Hu
Adobe PDF(1325Kb)  |  Favorite  |  View/Download:54/0  |  Submit date:2012/04/13
Dd-8  Single Crystal Alloy  Microstructural Stability  Alpha Chromium  Nickel-base Superalloy  Fatigue  
Influence of Co, W and Ti on the stress-rupture lives of a single crystal nickel-base superalloy 期刊论文
Journal of Materials Science & Technology, 2006, 卷号: 22, 期号: 2, 页码: 169-172
Authors:  D. Y. Yang;  T. Jin;  N. R. Zhao;  Z. H. Wang;  X. F. Sun;  H. R. Guan;  Z. Q. Hu
Favorite  |  View/Download:54/0  |  Submit date:2012/04/14
Nickel-base Single Crystal Superalloy  Orthogonal Array Design  Stress-rupture  Orthogonal Array Design  Optimization  Parameters  Alloy  
Antiphase boundary strengthening in a single crystal nickel-base superalloy 期刊论文
Journal of Materials Science & Technology, 2002, 卷号: 18, 期号: 2, 页码: 159-162
Authors:  J. H. Zhang;  T. Jin;  Y. B. Xu;  Z. Q. Hu;  X. Wu
Favorite  |  View/Download:57/0  |  Submit date:2012/04/14
Single Crystal Nickel-base Superalloy  Gamma' Phase  Strengthening  
Stress-induced precipitation of fine gamma '-phase and thermodynamics analysis 期刊论文
Journal of Materials Science & Technology, 2001, 卷号: 17, 期号: 2, 页码: 257-259
Authors:  S. G. Tian;  J. H. Zhang;  Y. B. Xu;  Z. Q. Hu;  H. C. Yang
Favorite  |  View/Download:75/0  |  Submit date:2012/04/14
Nickel-base Superalloy  Fatigue