Effect of solution heat treatment on creep properties of a nickel-based single crystal superalloy 期刊论文
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2021, 卷号: 15, 页码: 4702-4713
Authors:  Yunling, Du;  Yang, Yanhong;  Diao, Aimin;  Li, Yongmei;  Wang, Xinguang;  Zhou, Yizhou;  Li, Jinguo;  Sun, Xiaofeng
Favorite  |  View/Download:117/0  |  Submit date:2022/01/27
Nickel-based single crystal superalloys  Microstructural evolution  Creep behavior  Solution heat-treatment  
Co content dependence on the microstructure characteristic and creep performance at elevated temperature in Ru-containing single crystal superalloys 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 卷号: 825, 页码: 12
Authors:  Tan, Z. H.;  Wang, X. G.;  Cheng, Y.;  Li, Y. M.;  Yang, Y. H.;  Liu, J. L.;  Liu, J. D.;  Li, J. G.;  Zhou, Y. Z.;  Sun, X. F.
Favorite  |  View/Download:92/0  |  Submit date:2021/11/22
Ru-containing single crystal superalloys  Co  Creep property  Microstructural stability  Precipitates  
Co content dependence on the microstructure characteristic and creep performance at elevated temperature in Ru-containing single crystal superalloys 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 卷号: 825, 页码: 12
Authors:  Tan, Z. H.;  Wang, X. G.;  Cheng, Y.;  Li, Y. M.;  Yang, Y. H.;  Liu, J. L.;  Liu, J. D.;  Li, J. G.;  Zhou, Y. Z.;  Sun, X. F.
Favorite  |  View/Download:75/0  |  Submit date:2021/11/22
Ru-containing single crystal superalloys  Co  Creep property  Microstructural stability  Precipitates  
Effect of thermal exposure on the microstructure and creep properties of a fourth-generation Ni-based single crystal superalloy 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 卷号: 69, 页码: 180-187
Authors:  Huang, Yeshun;  Wang, Xinguang;  Cui, Chuanyong;  Tan, Zihao;  Li, Jinguo;  Yang, Yanhong;  Liu, Jinlai;  Zhou, Yizhou;  Sun, Xiaofeng
Favorite  |  View/Download:57/0  |  Submit date:2021/10/15
Ni-based single crystal superalloys  Thermal exposure  Microstructural evolution  Creep properties  Porosity  
Effect of thermal exposure on the microstructure and creep properties of a fourth-generation Ni-based single crystal superalloy 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 卷号: 69, 页码: 180-187
Authors:  Huang, Yeshun;  Wang, Xinguang;  Cui, Chuanyong;  Tan, Zihao;  Li, Jinguo;  Yang, Yanhong;  Liu, Jinlai;  Zhou, Yizhou;  Sun, Xiaofeng
Favorite  |  View/Download:60/0  |  Submit date:2021/10/15
Ni-based single crystal superalloys  Thermal exposure  Microstructural evolution  Creep properties  Porosity  
Influence of Geometric Structure and Feeding Behavior of Casting on Freckle Formation during Directional Solidification of a Ni-Based Single-Crystal Superalloy 期刊论文
CRYSTAL RESEARCH AND TECHNOLOGY, 2021, 页码: 11
Authors:  Han, Dongyu;  Jiang, Weiguo;  Xiao, Jiuhan;  Li, Kaiwen;  Lu, Yuzhang;  Lou, Langhong
Favorite  |  View/Download:71/0  |  Submit date:2021/10/15
casting structures  feeding behaviors  freckles  Ni‐  based superalloys  single crystal  
Influence of Geometric Structure and Feeding Behavior of Casting on Freckle Formation during Directional Solidification of a Ni-Based Single-Crystal Superalloy 期刊论文
CRYSTAL RESEARCH AND TECHNOLOGY, 2021, 页码: 11
Authors:  Han, Dongyu;  Jiang, Weiguo;  Xiao, Jiuhan;  Li, Kaiwen;  Lu, Yuzhang;  Lou, Langhong
Favorite  |  View/Download:67/0  |  Submit date:2021/10/15
casting structures  feeding behaviors  freckles  Ni‐  based superalloys  single crystal  
AN AB INITIO INVESTIGATION OF THE EFFECT OF Co, Ru, W, Ta ON THE STABILITY AND ELECTRONIC PROPERTIES OF Ni-BASE SINGLE CRYSTAL SUPERALLOYS 期刊论文
DIGEST JOURNAL OF NANOMATERIALS AND BIOSTRUCTURES, 2020, 卷号: 15, 期号: 4, 页码: 1215-1226
Authors:  Liu, J.;  Du, X.;  Li, J.
Favorite  |  View/Download:74/0  |  Submit date:2021/03/15
Site occupancy  Ab initio calculations  Ni-based single crystal superalloys  Electronic structure  
Effect of Ta on microstructural evolution of NiCrAlYSi coated Ni-base single crystal superalloys 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 卷号: 829, 页码: 14
Authors:  Yin, Bin;  Xie, Guang;  Lou, Langhong;  Zhang, Jian
Favorite  |  View/Download:75/0  |  Submit date:2021/02/02
Single crystal superalloys  NiCrAlYSi coating  Ta  Secondary reaction zone (SRZ)  Rafting  
Creep behavior and a deformation mechanism based creep rate model under high temperature and low stress condition for single crystal superalloy DD5 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 卷号: 786, 页码: 10
Authors:  Xu, Ke;  Wang, Guanglei;  Liu, Jide;  Li, Jinguo;  Liu, Jinlai;  Wang, Xinguang;  Yang, Yanhong;  Ye, Lihua;  Zhou, Yizhou;  Sun, Xiaofeng
Favorite  |  View/Download:80/0  |  Submit date:2021/02/02
Nickel based single crystal superalloys  Creep behavior  Microstructure  Creep model