Effects of microstructure evolution on the deformation mechanisms and tensile properties of a new Ni-base superalloy during aging at 800 degrees C 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 卷号: 68, 页码: 40-52
Authors:  Hou, Kunlei;  Wang, Min;  Ou, Meiqiong;  Li, Haoze;  Hao, Xianchao;  Ma, Yingche;  Liu, Kui
Favorite  |  View/Download:3/0  |  Submit date:2021/10/15
Ni-base superalloy  Aging  gamma ' size  Yield strength  Deformation mechanism  Fracture behavior  
Influence of Ta content on microstructure and creep behavior of a Ni-Co base disc superalloy 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 卷号: 802, 页码: 10
Authors:  Zhu, C. Z.;  Zhang, R.;  Cui, C. Y.;  Zhou, Y. Z.;  Liang, F. G.;  Liu, X.;  Sun, X. F.
Favorite  |  View/Download:2/0  |  Submit date:2021/10/15
Ni-Co base superalloy  Tantalum  Microstructure  Creep behavior  
Influence of Ta content on microstructure and creep behavior of a Ni-Co base disc superalloy 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 卷号: 802, 页码: 10
Authors:  Zhu, C. Z.;  Zhang, R.;  Cui, C. Y.;  Zhou, Y. Z.;  Liang, F. G.;  Liu, X.;  Sun, X. F.
Favorite  |  View/Download:3/0  |  Submit date:2021/10/15
Ni-Co base superalloy  Tantalum  Microstructure  Creep behavior  
Effect of Aspect Ratio on the Deformation Behavior of Dislocation-Free Ni3Al Nanocubes 期刊论文
NANOMATERIALS, 2020, 卷号: 10, 期号: 11, 页码: 11
Authors:  Li, Peng;  Wang, Xinguang;  Zhou, Yizhou;  Pfetzing-Micklich, Janine;  Somsen, Christoph;  Eggeler, Gunther
Favorite  |  View/Download:37/0  |  Submit date:2021/02/02
Ni3Al nanocubes  Ni-base superalloy single crystals  aspect ratio  in situ compression  dislocation free  
Effect of Aspect Ratio on the Deformation Behavior of Dislocation-Free Ni3Al Nanocubes 期刊论文
NANOMATERIALS, 2020, 卷号: 10, 期号: 11, 页码: 11
Authors:  Li, Peng;  Wang, Xinguang;  Zhou, Yizhou;  Pfetzing-Micklich, Janine;  Somsen, Christoph;  Eggeler, Gunther
Favorite  |  View/Download:35/0  |  Submit date:2021/02/02
Ni3Al nanocubes  Ni-base superalloy single crystals  aspect ratio  in situ compression  dislocation free  
Improving cyclic oxidation resistance of Ni3Al-based single crystal superalloy with low-diffusion platinum-modified aluminide coating 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2020, 卷号: 54, 页码: 132-143
Authors:  Liu, H.;  Xu, M. M.;  Li, S.;  Bao, Z. B.;  Zhu, S. L.;  Wang, F. H.
Favorite  |  View/Download:11/0  |  Submit date:2021/02/02
Ni3Al-base superalloy  Pt-modified aluminide coating  Re-rich diffusion barrier  Cyclic oxidation  Interdiffusion  Second reaction zone  
Improving cyclic oxidation resistance of Ni3Al-based single crystal superalloy with low-diffusion platinum-modified aluminide coating 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2020, 卷号: 54, 页码: 132-143
Authors:  Liu, H.;  Xu, M. M.;  Li, S.;  Bao, Z. B.;  Zhu, S. L.;  Wang, F. H.
Favorite  |  View/Download:10/0  |  Submit date:2021/02/02
Ni3Al-base superalloy  Pt-modified aluminide coating  Re-rich diffusion barrier  Cyclic oxidation  Interdiffusion  Second reaction zone  
Influence of Co content on the microstructures and mechanical properties of a Ni-Co base superalloy made by specific additive manufacturing process 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 卷号: 786, 页码: 10
Authors:  Tang, Ling;  Liang, Jingjing;  Cui, Chuanyong;  Li, Jinguo;  Zhou, Yizhou;  Sun, Xiaofeng;  Ding, Yutian
Favorite  |  View/Download:12/0  |  Submit date:2021/02/02
Additive manufacturing  Ni-Co base Superalloy  Tensile strength  Deformation mechanism  
Effect of Rejuvenation Heat Treatment on the Creep Property and Microstructural Evolution of a Ni-Base Superalloy 期刊论文
APPLIED SCIENCES-BASEL, 2020, 卷号: 10, 期号: 3, 页码: 13
Authors:  Wang, Linning;  Liu, Yuan;  Liang, Jingjing
Favorite  |  View/Download:9/0  |  Submit date:2021/02/02
Ni-base superalloy  rejuvenation treatment  creep  carbides  gamma ' precipitates  
Effect of Rejuvenation Heat Treatment on the Creep Property and Microstructural Evolution of a Ni-Base Superalloy 期刊论文
APPLIED SCIENCES-BASEL, 2020, 卷号: 10, 期号: 3, 页码: 13
Authors:  Wang, Linning;  Liu, Yuan;  Liang, Jingjing
Favorite  |  View/Download:12/0  |  Submit date:2021/02/02
Ni-base superalloy  rejuvenation treatment  creep  carbides  gamma ' precipitates