IMR OpenIR

Browse/Search Results:  1-10 of 132 Help

Selected(0)Clear Items/Page:    Sort:
Effect of pre-strain treatment on mechanical properties of a Ni-Co base disk superalloy 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 卷号: 905, 页码: 10
Authors:  Zhu, C. Z.;  Zhang, R.;  Cui, C. Y.;  Zhou, Y. Z.;  Qu, J. L.;  Gan, B.;  Zhang, B. J.;  Sun, X. F.
Favorite  |  View/Download:11/0  |  Submit date:2022/07/01
Ni-Co base superalloy  Pre-strain  Microstructure  Mechanical property  Microtwinning  Suzuki segregation  
Evolution of Interfacial Microstructure of Ni-Co Base Superalloy During Plastic Deformation Bonding and Its Bonding Mechanism 期刊论文
ACTA METALLURGICA SINICA, 2022, 卷号: 58, 期号: 2, 页码: 129-140
Authors:  Ren Shaofei;  Zhang Jianyang;  Zhang Xinfang;  Sun Mingyue;  Xu Bin;  Cui Chuanyong
Favorite  |  View/Download:8/0  |  Submit date:2022/07/01
Ni-Co base superalloy  plastic deformation bonding  dynamic recrystallization  
Effect of grain boundary precipitates on the stress rupture properties of K4750 alloy after long-term aging at 750 degrees C for 8000 h 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 卷号: 92, 页码: 11-20
Authors:  Ou, Meiqiong;  Ma, Yingche;  Hou, Kunlei;  Wang, Min;  Ma, Guangcai;  Liu, Kui
Favorite  |  View/Download:36/0  |  Submit date:2022/01/27
Ni-base superalloy  Long-term aging, MC carbide  eta phase  Stress rupture properties  Residual strain distribution  
Effects of microstructure evolution on the deformation mechanisms and tensile properties of a new Ni-base superalloy during aging at 800 degrees C 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 卷号: 68, 页码: 40-52
Authors:  Hou, Kunlei;  Wang, Min;  Ou, Meiqiong;  Li, Haoze;  Hao, Xianchao;  Ma, Yingche;  Liu, Kui
Favorite  |  View/Download:26/0  |  Submit date:2021/10/15
Ni-base superalloy  Aging  gamma ' size  Yield strength  Deformation mechanism  Fracture behavior  
Influence of Ta content on microstructure and creep behavior of a Ni-Co base disc superalloy 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 卷号: 802, 页码: 10
Authors:  Zhu, C. Z.;  Zhang, R.;  Cui, C. Y.;  Zhou, Y. Z.;  Liang, F. G.;  Liu, X.;  Sun, X. F.
Favorite  |  View/Download:25/0  |  Submit date:2021/10/15
Ni-Co base superalloy  Tantalum  Microstructure  Creep behavior  
Influence of Ta content on microstructure and creep behavior of a Ni-Co base disc superalloy 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 卷号: 802, 页码: 10
Authors:  Zhu, C. Z.;  Zhang, R.;  Cui, C. Y.;  Zhou, Y. Z.;  Liang, F. G.;  Liu, X.;  Sun, X. F.
Favorite  |  View/Download:26/0  |  Submit date:2021/10/15
Ni-Co base superalloy  Tantalum  Microstructure  Creep behavior  
Effect of Aspect Ratio on the Deformation Behavior of Dislocation-Free Ni3Al Nanocubes 期刊论文
NANOMATERIALS, 2020, 卷号: 10, 期号: 11, 页码: 11
Authors:  Li, Peng;  Wang, Xinguang;  Zhou, Yizhou;  Pfetzing-Micklich, Janine;  Somsen, Christoph;  Eggeler, Gunther
Favorite  |  View/Download:104/0  |  Submit date:2021/02/02
Ni3Al nanocubes  Ni-base superalloy single crystals  aspect ratio  in situ compression  dislocation free  
Effect of Aspect Ratio on the Deformation Behavior of Dislocation-Free Ni3Al Nanocubes 期刊论文
NANOMATERIALS, 2020, 卷号: 10, 期号: 11, 页码: 11
Authors:  Li, Peng;  Wang, Xinguang;  Zhou, Yizhou;  Pfetzing-Micklich, Janine;  Somsen, Christoph;  Eggeler, Gunther
Favorite  |  View/Download:99/0  |  Submit date:2021/02/02
Ni3Al nanocubes  Ni-base superalloy single crystals  aspect ratio  in situ compression  dislocation free  
Improving cyclic oxidation resistance of Ni3Al-based single crystal superalloy with low-diffusion platinum-modified aluminide coating 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2020, 卷号: 54, 页码: 132-143
Authors:  Liu, H.;  Xu, M. M.;  Li, S.;  Bao, Z. B.;  Zhu, S. L.;  Wang, F. H.
Favorite  |  View/Download:38/0  |  Submit date:2021/02/02
Ni3Al-base superalloy  Pt-modified aluminide coating  Re-rich diffusion barrier  Cyclic oxidation  Interdiffusion  Second reaction zone  
Improving cyclic oxidation resistance of Ni3Al-based single crystal superalloy with low-diffusion platinum-modified aluminide coating 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2020, 卷号: 54, 页码: 132-143
Authors:  Liu, H.;  Xu, M. M.;  Li, S.;  Bao, Z. B.;  Zhu, S. L.;  Wang, F. H.
Favorite  |  View/Download:38/0  |  Submit date:2021/02/02
Ni3Al-base superalloy  Pt-modified aluminide coating  Re-rich diffusion barrier  Cyclic oxidation  Interdiffusion  Second reaction zone