Effects of reduced sulfur on passive film properties of steam generator (SG) tubing: an overview
Xia, Da-Hai1,2,3; Luo, Jing-Li3
Corresponding AuthorXia, Da-Hai(dahaixia@tju.edu.cn) ; Luo, Jing-Li(jingli_luo@ualberta.ca)
2019-05-07
Source PublicationANTI-CORROSION METHODS AND MATERIALS
ISSN0003-5599
Volume66Issue:3Pages:317-326
AbstractPurpose Corrosion is considered as one of the issues that threaten the safe operation of steam generator (SG) tubing. Some sulfur-related specie can cause corrosion degradation of SG tubing. Sulfur-induced corrosion of SG alloys in high temperature and high-pressure water is one of the most complicated processes. The purpose of this study is to study the effect of reduced sulphur on passive film properties of steam generator (SG) tubing. Design/methodology/approach In this paper, the effects of reduced sulfur on passive film properties of SG tubing were reviewed from the aspects of thermodynamic calculations and experimental. Findings Thermodynamic calculations are mainly presented by E-pH diagrams, volt equivalent diagrams and species distribution curves. The stability of sulphur species highly depends on temperature, solution pH, and electrochemical potential. Experimental data indicated that reduced sulfur species can interact with the passive film, which led to changes in film thickness, film structure, semiconductivity and pitting growth rate. Originality/value The state-of-the-art discussed in this paper gives basis for resolving engineering problems regarding with sulfur-induced corrosion.
KeywordCorrosion Passive film Steam generator Sulphide Tetrathionate Thiosulphate
Funding OrganizationNational Natural Science Foundation of China ; open-ended fund of the CAS Key laboratory of Nuclear Materials and Safety Assessment (Institute of Metal Research, Chinese Academy of Sciences, China)
DOI10.1108/ACMM-09-2018-1996
Indexed BySCI
Language英语
Funding ProjectNational Natural Science Foundation of China[51701140] ; open-ended fund of the CAS Key laboratory of Nuclear Materials and Safety Assessment (Institute of Metal Research, Chinese Academy of Sciences, China)[2018NMSAKF01]
WOS Research AreaMetallurgy & Metallurgical Engineering
WOS SubjectMetallurgy & Metallurgical Engineering
WOS IDWOS:000465588100007
PublisherEMERALD GROUP PUBLISHING LTD
Citation statistics
Cited Times:7[WOS]   [WOS Record]     [Related Records in WOS]
Document Type期刊论文
Identifierhttp://ir.imr.ac.cn/handle/321006/133035
Collection中国科学院金属研究所
Corresponding AuthorXia, Da-Hai; Luo, Jing-Li
Affiliation1.Tianjin Univ, Tianjin Key Lab Composite & Funct Mat, Sch Mat Sci & Engn, Tianjin, Peoples R China
2.Chinese Acad Sci, Inst Met Res, Shenyang, Liaoning, Peoples R China
3.Univ Alberta, Dept Chem & Mat Engn, Edmonton, AB, Canada
Recommended Citation
GB/T 7714
Xia, Da-Hai,Luo, Jing-Li. Effects of reduced sulfur on passive film properties of steam generator (SG) tubing: an overview[J]. ANTI-CORROSION METHODS AND MATERIALS,2019,66(3):317-326.
APA Xia, Da-Hai,&Luo, Jing-Li.(2019).Effects of reduced sulfur on passive film properties of steam generator (SG) tubing: an overview.ANTI-CORROSION METHODS AND MATERIALS,66(3),317-326.
MLA Xia, Da-Hai,et al."Effects of reduced sulfur on passive film properties of steam generator (SG) tubing: an overview".ANTI-CORROSION METHODS AND MATERIALS 66.3(2019):317-326.
Files in This Item:
There are no files associated with this item.
Related Services
Recommend this item
Bookmark
Usage statistics
Export to Endnote
Google Scholar
Similar articles in Google Scholar
[Xia, Da-Hai]'s Articles
[Luo, Jing-Li]'s Articles
Baidu academic
Similar articles in Baidu academic
[Xia, Da-Hai]'s Articles
[Luo, Jing-Li]'s Articles
Bing Scholar
Similar articles in Bing Scholar
[Xia, Da-Hai]'s Articles
[Luo, Jing-Li]'s Articles
Terms of Use
No data!
Social Bookmark/Share
All comments (0)
No comment.
 

Items in the repository are protected by copyright, with all rights reserved, unless otherwise indicated.