Abstract | 目的micro—CT评价新型低弹βB钛合金内植物对大鼠骨质疏松骨折愈合的作用及应力遮挡效应。方法SD雌性大鼠去势,建立骨质疏松动物模型,采用Utvag方法制备双股骨骨折模型,选用弹性模量分别为110GPa和30GPa的钛合金制成髓内针固定骨折,左侧为高弹组,右侧为低弹组,分别于术后2、4、6、12w行micro—CT测定,检测骨小梁的体积(BV)、样本体积(TV)、骨体积分数(BVF)、骨小梁间隙(Tb.Sp)、骨小梁厚度(Tb.Th)、骨小梁数(Tb.N)和结构模型指数(SMI)等指标,比较两种弹性模量钛合金植入物对骨折骨痂形成的影响,并进行统计学分析。结果骨质疏松大鼠股骨骨折后4w,兴趣区域1(ROI1)区,低弹组除TV、Tb.Sp高于高弹组外,BV、BVF、Tb,Th均低于高弹组;术后6w,ROI1区,低弹组TV值高于高弹组,其余差异无显著性;术后12w,ROI1区,低弹组TV、BV、Tb.N、Tb.Th、SMI均高于高弹组。ROI2区,低弹组BV、BVF、SMI均高于高弹组。结论新型低弹β钛合金内植物有利于大鼠骨质疏松骨折早期骨痂的形成,并提高骨折愈合的远期质量,减少了骨折固定节段的骨量丢失。 |
Other Abstract | Objective To investigate the influence of the low-modulus of elasticity (30 GPa) fixation on bone healing of osteoporotie fracture and the effects of stress shielding by miero-CT. Methods Thirty female Sprague- Dawley rats, aged 3 months, were selected, OVX was performed twelve weeks before femur fracture, the fracture of left femur was stabilized with the high-modulus of elasticity titanium alloy pin and the right with the low-modulus of elasticity. The bony calluses were observed miero-CT at two, four, six, and twelve weeks after fracture. The parameters included BV, TV, BVF, Tb. Th, Tb. N, Tb. Sp, SMI. Results The calluses at the low-modulus of elasticity group showed a significantly lower percentage of mineralized bone at 2 - 4 weeks postoperatively, and a higher amount of fibrous callus than the high-modulus of elasticity group. The calluses were no longer distinguishable at 6 - 9 weeks. The superior trabecular bone mierostructure was produced and less bone loss were shown under the low-modulus of elasticity pin at 12 weeks. Conclusion The new low elastic modulus β Ti alloy seemed to increase the fibrous callus formation at the initial phase, and improve the quality of bone healing at the later phase. |
Keyword | 弹性模量 钛合金 micro—CT 骨质疏松性骨折 |
Indexed By | CSCD |
Language | 中文 |
CSCD ID | CSCD:2978918 |
Citation statistics | |
Document Type | 期刊论文 |
Identifier | http://ir.imr.ac.cn/handle/321006/143162 |
Collection | 中国科学院金属研究所 |
Affiliation | 中国科学院金属研究所 |
Recommended Citation GB/T 7714 | 沙漠,郭征,付军,等. Micro—CT评价新型低弹β钛合金对动物骨质疏松性骨折愈合的影响[J]. 中国骨质疏松杂志,2007,13.0(010):704-708. |
APA | 沙漠.,郭征.,付军.,李述军.,李靖.,...&王军.(2007).Micro—CT评价新型低弹β钛合金对动物骨质疏松性骨折愈合的影响.中国骨质疏松杂志,13.0(010),704-708. |
MLA | 沙漠,et al."Micro—CT评价新型低弹β钛合金对动物骨质疏松性骨折愈合的影响".中国骨质疏松杂志 13.0.010(2007):704-708. |
Files in This Item: | There are no files associated with this item. |
Items in the repository are protected by copyright, with all rights reserved, unless otherwise indicated.
Edit Comment