IMR OpenIR
超高纯铁素体不锈钢在3.5%—NaCl中的腐蚀疲劳的裂纹萌生
王俭秋; 李劲; 王政富; 朱自勇; 柯伟; 臧启山; 王中光
1995
Source Publication金属学报
ISSN0412-1961
Volume31.0Issue:003Pages:B103-B108
Keyword低周疲劳 裂纹萌生 点蚀 铁素体不锈钢 腐蚀疲劳
Indexed ByCSCD
Language中文
CSCD IDCSCD:938999
Citation statistics
Document Type期刊论文
Identifierhttp://ir.imr.ac.cn/handle/321006/148879
Collection中国科学院金属研究所
Affiliation中国科学院金属研究所
Recommended Citation
GB/T 7714
王俭秋,李劲,王政富,等. 超高纯铁素体不锈钢在3.5%—NaCl中的腐蚀疲劳的裂纹萌生[J]. 金属学报,1995,31.0(003):B103-B108.
APA 王俭秋.,李劲.,王政富.,朱自勇.,柯伟.,...&王中光.(1995).超高纯铁素体不锈钢在3.5%—NaCl中的腐蚀疲劳的裂纹萌生.金属学报,31.0(003),B103-B108.
MLA 王俭秋,et al."超高纯铁素体不锈钢在3.5%—NaCl中的腐蚀疲劳的裂纹萌生".金属学报 31.0.003(1995):B103-B108.
Files in This Item:
There are no files associated with this item.
Related Services
Recommend this item
Bookmark
Usage statistics
Export to Endnote
Google Scholar
Similar articles in Google Scholar
[王俭秋]'s Articles
[李劲]'s Articles
[王政富]'s Articles
Baidu academic
Similar articles in Baidu academic
[王俭秋]'s Articles
[李劲]'s Articles
[王政富]'s Articles
Bing Scholar
Similar articles in Bing Scholar
[王俭秋]'s Articles
[李劲]'s Articles
[王政富]'s Articles
Terms of Use
No data!
Social Bookmark/Share
All comments (0)
No comment.
 

Items in the repository are protected by copyright, with all rights reserved, unless otherwise indicated.