超高纯铁素体不锈钢在3.5%—NaCl中的腐蚀疲劳的裂纹萌生 | |
王俭秋; 李劲; 王政富; 朱自勇; 柯伟; 臧启山; 王中光 | |
1995 | |
Source Publication | 金属学报
![]() |
ISSN | 0412-1961 |
Volume | 31.0Issue:003Pages:B103-B108 |
Keyword | 低周疲劳 裂纹萌生 点蚀 铁素体不锈钢 腐蚀疲劳 |
Indexed By | CSCD |
Language | 中文 |
CSCD ID | CSCD:938999 |
Citation statistics | |
Document Type | 期刊论文 |
Identifier | http://ir.imr.ac.cn/handle/321006/148881 |
Collection | 中国科学院金属研究所 |
Affiliation | 中国科学院金属研究所 |
Recommended Citation GB/T 7714 | 王俭秋,李劲,王政富,等. 超高纯铁素体不锈钢在3.5%—NaCl中的腐蚀疲劳的裂纹萌生[J]. 金属学报,1995,31.0(003):B103-B108. |
APA | 王俭秋.,李劲.,王政富.,朱自勇.,柯伟.,...&王中光.(1995).超高纯铁素体不锈钢在3.5%—NaCl中的腐蚀疲劳的裂纹萌生.金属学报,31.0(003),B103-B108. |
MLA | 王俭秋,et al."超高纯铁素体不锈钢在3.5%—NaCl中的腐蚀疲劳的裂纹萌生".金属学报 31.0.003(1995):B103-B108. |