Effect of solution treatment on microstructure evolution and mechanical properties of Mg-6.0Zn-0.6Y-0.5Zr alloy processed by equal channel angular extrusion; Effect of solution treatment on microstructure evolution and mechanical properties of Mg-6.0Zn-0.6Y-0.5Zr alloy processed by equal channel angular extrusion
W. N. Tang; R. S. Chen; E. H. Han
2008 ; 2008
发表期刊Materials Transactions ; Materials Transactions
ISSN1345-9678 ; 1345-9678
卷号49期号:5页码:957-962
摘要The effect of solution treatment before equal channel angular extrusion (ECAE) on the evolution of microstructures and mechanical properties in as-cast Mg-6.0Zn-0.6Y-0.5Zr alloy after different ECAE passes has been systematically investigated. The micrographs and tensile results showed that the solution treatment significantly influenced the microstructural evolution, as well as tensile strength and elongation. ECAE processing results in producing finer grain structure both in the as-cast and as-solutionized alloys when the passes increased. However, solution treatment before ECAE provides a significant increase in forming rate of fine recrystallized grains during ECAE at high temperature of 623 K. A fully recrystallized microstructure was observed after 8 passes in the as-solutionized alloy, while it was not finished even after 8 passes in the as-cast alloy. The ductility of as-solutionized alloy is always significantly better than those of the as-cast alloy. However, the strengths of the former are better than those of the later only after the passes beyond 6 passes.; The effect of solution treatment before equal channel angular extrusion (ECAE) on the evolution of microstructures and mechanical properties in as-cast Mg-6.0Zn-0.6Y-0.5Zr alloy after different ECAE passes has been systematically investigated. The micrographs and tensile results showed that the solution treatment significantly influenced the microstructural evolution, as well as tensile strength and elongation. ECAE processing results in producing finer grain structure both in the as-cast and as-solutionized alloys when the passes increased. However, solution treatment before ECAE provides a significant increase in forming rate of fine recrystallized grains during ECAE at high temperature of 623 K. A fully recrystallized microstructure was observed after 8 passes in the as-solutionized alloy, while it was not finished even after 8 passes in the as-cast alloy. The ductility of as-solutionized alloy is always significantly better than those of the as-cast alloy. However, the strengths of the former are better than those of the later only after the passes beyond 6 passes.
部门归属[tang, weineng; chen, rongshi; han, enhou] chinese acad sci, inst met res, environm corros ctr, shenyang 110016, peoples r china. [tang, weineng] chinese acad sci, grad sch, beijing 100864, peoples r china.;chen, rs (reprint author), chinese acad sci, inst met res, environm corros ctr, shenyang 110016, peoples r china;rschen@imr.ac.cn ; [tang, weineng; chen, rongshi; han, enhou] chinese acad sci, inst met res, environm corros ctr, shenyang 110016, peoples r china. [tang, weineng] chinese acad sci, grad sch, beijing 100864, peoples r china.;chen, rs (reprint author), chinese acad sci, inst met res, environm corros ctr, shenyang 110016, peoples r china;rschen@imr.ac.cn
关键词Ecae Ecae Solution Treatment Solution Treatment Magnesium-zinc-yttrium Magnesium-zinc-yttrium Microstructure Microstructure Mechanical Properties Mechanical Properties Zn-y Alloys Zn-y Alloys Quasi-crystalline Particles Quasi-crystalline Particles Coarse 2nd-phase Particles Coarse 2nd-phase Particles Az31 Magnesium Alloy Az31 Magnesium Alloy Deformation-behavior Deformation-behavior Zr Alloy Zr Alloy Mg Mg Superplasticity Superplasticity Phase Phase Temperature Temperature
URL查看原文 ; 查看原文
WOS记录号WOS:000256950400014 ; WOS:000256950400014
引用统计
被引频次:2[WOS]   [WOS记录]     [WOS相关记录]
文献类型期刊论文
条目标识符http://ir.imr.ac.cn/handle/321006/33099
专题中国科学院金属研究所
推荐引用方式
GB/T 7714
W. N. Tang,R. S. Chen,E. H. Han. Effect of solution treatment on microstructure evolution and mechanical properties of Mg-6.0Zn-0.6Y-0.5Zr alloy processed by equal channel angular extrusion, Effect of solution treatment on microstructure evolution and mechanical properties of Mg-6.0Zn-0.6Y-0.5Zr alloy processed by equal channel angular extrusion[J]. Materials Transactions, Materials Transactions,2008, 2008,49, 49(5):957-962, 957-962.
APA W. N. Tang,R. S. Chen,&E. H. Han.(2008).Effect of solution treatment on microstructure evolution and mechanical properties of Mg-6.0Zn-0.6Y-0.5Zr alloy processed by equal channel angular extrusion.Materials Transactions,49(5),957-962.
MLA W. N. Tang,et al."Effect of solution treatment on microstructure evolution and mechanical properties of Mg-6.0Zn-0.6Y-0.5Zr alloy processed by equal channel angular extrusion".Materials Transactions 49.5(2008):957-962.
条目包含的文件
文件名称/大小 文献类型 版本类型 开放类型 使用许可
453.pdf(521KB) 开放获取--
个性服务
推荐该条目
保存到收藏夹
查看访问统计
导出为Endnote文件
谷歌学术
谷歌学术中相似的文章
[W. N. Tang]的文章
[R. S. Chen]的文章
[E. H. Han]的文章
百度学术
百度学术中相似的文章
[W. N. Tang]的文章
[R. S. Chen]的文章
[E. H. Han]的文章
必应学术
必应学术中相似的文章
[W. N. Tang]的文章
[R. S. Chen]的文章
[E. H. Han]的文章
相关权益政策
暂无数据
收藏/分享
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。