| Evolution of oxide scale morphology on (Ni,Pd)Al coating during high temperature oxidation in air |
| Guan, HR; Li, MJ; Sun, XF
|
通讯作者 | Guan, HR(hrguan@imr.ac.cn)
|
| 2004
|
发表期刊 | HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS
 |
ISSN | 0255-5476
|
卷号 | 461-464页码:417-423 |
摘要 | The morphology evolution of oxide scale formed on the (Ni,Pd)AI coating during oxidation in air at 900 similar to 1100degreesC was investigated systematically by scanning electron microscope and XRD. A long-term observation showed that the transformation of theta- to alpha-Al2O3 occurred on the (Ni,Pd)Al coating with increasing oxidation temperature and time. Furthermore, such transformation is more rapid on the (Ni,Pd)Al coating in comparison to a simple NiAl coating. In addition, the various morphologies for the theta-Al2O3 are also presented in this paper. |
关键词 | (Ni,Pd)Al coating
high temperature oxidation
transformation
theta-Al2O3
alpha-Al2O3
|
收录类别 | SCI
|
语种 | 英语
|
WOS研究方向 | Materials Science
; Metallurgy & Metallurgical Engineering
|
WOS类目 | Materials Science, Multidisciplinary
; Metallurgy & Metallurgical Engineering
|
WOS记录号 | WOS:000223339700051
|
出版者 | TRANS TECH PUBLICATIONS LTD
|
引用统计 |
|
文献类型 | 期刊论文
|
条目标识符 | http://ir.imr.ac.cn/handle/321006/81415
|
专题 | 中国科学院金属研究所
|
通讯作者 | Guan, HR |
作者单位 | Chinese Acad Sci, Inst Met Res, Shenyang R&D Ctr Adv Mat, Superalloy Res Div, Shenyang 110016, Peoples R China
|
推荐引用方式 GB/T 7714 |
Guan, HR,Li, MJ,Sun, XF. Evolution of oxide scale morphology on (Ni,Pd)Al coating during high temperature oxidation in air[J]. HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS,2004,461-464:417-423.
|
APA |
Guan, HR,Li, MJ,&Sun, XF.(2004).Evolution of oxide scale morphology on (Ni,Pd)Al coating during high temperature oxidation in air.HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS,461-464,417-423.
|
MLA |
Guan, HR,et al."Evolution of oxide scale morphology on (Ni,Pd)Al coating during high temperature oxidation in air".HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS 461-464(2004):417-423.
|
修改评论