Atmospheric corrosion of A3 steel deposited with different salts
Wan, Y; Yan, CW; Cao, CN
通讯作者Wan, Y(ywan@imr.ac.cn)
2004-06-01
发表期刊ACTA PHYSICO-CHIMICA SINICA
ISSN1000-6818
卷号20期号:6页码:659-663
摘要The atmospheric corrosion of A3 steel with Na2SO4,(NH4) SO4,NH4Cl and NaCl deposited on it has been investigated at 298 K with relative humidity of (85 +/- 5) %. The results show: that A3 steel deposited by the salts corroded more and more seriously as the corrosion time went on and metal loss obeys the equation of Deltam/ A = K . t(h). FTIR, SEM and XRD were utilized to study the development and characterization of corrosion products, and the results indicate that A3 steel with the salts deposited corroded much faster than the blank samples, and the corrosion of A3 steel initialed along the deposition area of the salts.
关键词steel A3 salt deposition atmospheric corrosion
DOI10.3866/PKU.WHXB20040622
收录类别SCI
语种英语
WOS研究方向Chemistry
WOS类目Chemistry, Physical
WOS记录号WOS:000222223400022
出版者PEKING UNIV PRESS
引用统计
文献类型期刊论文
条目标识符http://ir.imr.ac.cn/handle/321006/82016
通讯作者Wan, Y
作者单位Chinese Acad Sci, Inst Met Res, State Key Lab Corros & Protect, Shenyang 110016, Peoples R China
推荐引用方式
GB/T 7714
Wan, Y,Yan, CW,Cao, CN. Atmospheric corrosion of A3 steel deposited with different salts[J]. ACTA PHYSICO-CHIMICA SINICA,2004,20(6):659-663.
APA Wan, Y,Yan, CW,&Cao, CN.(2004).Atmospheric corrosion of A3 steel deposited with different salts.ACTA PHYSICO-CHIMICA SINICA,20(6),659-663.
MLA Wan, Y,et al."Atmospheric corrosion of A3 steel deposited with different salts".ACTA PHYSICO-CHIMICA SINICA 20.6(2004):659-663.
条目包含的文件
条目无相关文件。
个性服务
推荐该条目
保存到收藏夹
查看访问统计
导出为Endnote文件
谷歌学术
谷歌学术中相似的文章
[Wan, Y]的文章
[Yan, CW]的文章
[Cao, CN]的文章
百度学术
百度学术中相似的文章
[Wan, Y]的文章
[Yan, CW]的文章
[Cao, CN]的文章
必应学术
必应学术中相似的文章
[Wan, Y]的文章
[Yan, CW]的文章
[Cao, CN]的文章
相关权益政策
暂无数据
收藏/分享
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。