Preferential growth of helium-doped Ti films deposited by magnetron sputtering
Zhang, Lei1; Shi, L. Q.1; He, Z. J.1; Zhang, B.1; Wang, L. B.2
Corresponding AuthorShi, L. Q.(lqshi@fudan.edu.cn)
2009-11-01
Source PublicationJOURNAL OF VACUUM SCIENCE & TECHNOLOGY A
ISSN0734-2101
Volume27Issue:6Pages:1392-1399
AbstractThe authors present a study on the influence of the bias voltages on the preferred orientation and microstructure of helium-doped Ti films. The films were deposited in a vacuum chamber by both direct-current magnetron sputtering and electron-cyclotron-resonance plasma-aided magnetron sputtering (ECR-PMS) methods. The preferred orientation and microstructure of the films were analyzed by x-ray diffraction (XRD) and transmission electron microscopy. They found that the preferred crystal orientation of helium-doped Ti films was controllably varied from (002) to (100) orientation by increasing the bias voltage (i.e., ion bombardment current and energy). The dominant bombardment effect on the orientation was from the Ar ions of the anode sheath in the magnetron sputtering plasma, and He bombardment also showed a slight influence on the orientation transformation at low trapped-helium content in the crystal. The XRD peak broadening of helium-doped Ti films prepared by ECR-PMS is much more serious than for conventional magnetron sputtering even at low helium concentrations. It is believed that asynchronous bombardment from He ions in the ECR plasma area and Ar ions in the deposition plasma during film growth significantly decreases the mobility of Ti adatoms on the surface and enhances the growth of helium-induced defects, thus increasing the crystal disorder and influencing the crystal orientation transformation. On the contrary, the sequential bombardment of He and Ar particles can decrease helium-dissolution produced defects and improve crystallization. (C) 2009 American Vacuum Society. [DOI: 10.1116/1.3253087]
Funding OrganizationNational Nature Science Foundation of China ; Shanghai Leading Academic Discipline Project
DOI10.1116/1.3253087
Indexed BySCI
Language英语
Funding ProjectNational Nature Science Foundation of China[10675034] ; National Nature Science Foundation of China[10475016] ; Shanghai Leading Academic Discipline Project[B107]
WOS Research AreaMaterials Science ; Physics
WOS SubjectMaterials Science, Coatings & Films ; Physics, Applied
WOS IDWOS:000271284500021
PublisherA V S AMER INST PHYSICS
Citation statistics
Document Type期刊论文
Identifierhttp://ir.imr.ac.cn/handle/321006/97543
Collection中国科学院金属研究所
Corresponding AuthorShi, L. Q.
Affiliation1.Fudan Univ, Inst Modern Phys, Appl Ion Beam Phys Lab, Shanghai 200433, Peoples R China
2.Chinese Acad Sci, Inst Met Phys, Shenyang 110016, Peoples R China
Recommended Citation
GB/T 7714
Zhang, Lei,Shi, L. Q.,He, Z. J.,et al. Preferential growth of helium-doped Ti films deposited by magnetron sputtering[J]. JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A,2009,27(6):1392-1399.
APA Zhang, Lei,Shi, L. Q.,He, Z. J.,Zhang, B.,&Wang, L. B..(2009).Preferential growth of helium-doped Ti films deposited by magnetron sputtering.JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A,27(6),1392-1399.
MLA Zhang, Lei,et al."Preferential growth of helium-doped Ti films deposited by magnetron sputtering".JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A 27.6(2009):1392-1399.
Files in This Item:
There are no files associated with this item.
Related Services
Recommend this item
Bookmark
Usage statistics
Export to Endnote
Google Scholar
Similar articles in Google Scholar
[Zhang, Lei]'s Articles
[Shi, L. Q.]'s Articles
[He, Z. J.]'s Articles
Baidu academic
Similar articles in Baidu academic
[Zhang, Lei]'s Articles
[Shi, L. Q.]'s Articles
[He, Z. J.]'s Articles
Bing Scholar
Similar articles in Bing Scholar
[Zhang, Lei]'s Articles
[Shi, L. Q.]'s Articles
[He, Z. J.]'s Articles
Terms of Use
No data!
Social Bookmark/Share
All comments (0)
No comment.
 

Items in the repository are protected by copyright, with all rights reserved, unless otherwise indicated.