IMR OpenIR

浏览/检索结果: 共194条,第1-10条 帮助

已选(0)清除 条数/页:   排序方式:
Planar slip triggered by successive dislocation-precipitate interaction in titanium alloys 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 卷号: 882, 页码: 6
作者:  Guo, H.;  Zhang, M. M.;  Xu, D. S.;  Zhang, J. H.;  Qiu, J. K.;  Meng, Z. C.;  Zheng, S. J.;  Ma, Y. J.;  Wang, H.;  Yang, R.
收藏  |  浏览/下载:12/0  |  提交时间:2024/01/08
Planar slip  Molecular dynamics  a(2) phase  Anti-phase boundary  Titanium  
Achieving superior fatigue strength in a powder-metallurgy titanium alloy via in-situ globularization during hot isostatic pressing 期刊论文
SCRIPTA MATERIALIA, 2023, 卷号: 228, 页码: 6
作者:  Guo, R. P.;  Cheng, M.;  Zhang, C. J.;  Qiao, J. W.;  Cai, C.;  Wang, Q. J.;  Xu, D. S.;  Xu, L.;  Yang, R.;  Shi, Y. S.;  Liaw, P. K.
收藏  |  浏览/下载:12/0  |  提交时间:2024/01/07
Titanium alloys  Hot isostatic pressing  Globularization  Fatigue strength  Fatigue-crack initiation  
Achievement of high strength and plasticity product of the nugget zone in friction stir welded high-Mn steel via controlling stacking fault energy 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 卷号: 862, 页码: 12
作者:  Wang, Y. Q.;  Guo, S.;  Duan, R. H.;  Luo, Z. A.;  Chen, J.;  Ma, Z. Y.;  Xie, G. M.
收藏  |  浏览/下载:48/0  |  提交时间:2023/05/09
Friction stir welding  High Mn steel  Preheating  Stacking fault energy  TWIP effect  
Enhancing wear resistance of TiN coating by gradient bias voltage and arc-enhanced glow discharge 期刊论文
CERAMICS INTERNATIONAL, 2022, 卷号: 48, 期号: 6, 页码: 8746-8750
作者:  Wang, Y. H.;  Guo, F.;  Ren, H.;  Hu, S. Y.;  Chen, Y. J.;  Zhao, Y. H.;  Gong, F.;  Xie, Z. W.
收藏  |  浏览/下载:114/0  |  提交时间:2022/07/01
TiN coating  Arc ion plating  Arc-enhanced glow discharge  Gradient bias  Wear  
Failure analysis of screw shaft in screw compressor 期刊论文
ENGINEERING FAILURE ANALYSIS, 2021, 卷号: 125, 页码: 10
作者:  Wang, M. S.;  Jia, X. D.;  Lv, W. Y.;  Sun, W. H.;  Bai, F. X.;  Guo, H.
收藏  |  浏览/下载:124/0  |  提交时间:2021/10/15
Screw compressor  Screw shaft  Failure analysis  Fatigue fracture  
TEM study on the morphology and interface microstructure of C/C-SiC composites fabricated by liquid infiltration 期刊论文
MATERIALS CHARACTERIZATION, 2021, 卷号: 175, 页码: 7
作者:  Zhang, K. X.;  Guo, X. S.;  Cheng, Y. X.;  Zhang, F. Q.;  He, L. L.
收藏  |  浏览/下载:114/0  |  提交时间:2021/10/15
Composites  C  C-SiC  Liquid silicon infiltration  TEM  Morphology  Interfacial microstructure  
The corrosion behavior of Ni-Cr-Al alloys exposed to mixed oxidizing- carburizing atmospheres at 800 degrees C 期刊论文
CORROSION SCIENCE, 2020, 卷号: 176
作者:  Guo, X. H.;  Shen, J.;  Liu, S.;  Chen, J.;  Niu, Y.
收藏  |  浏览/下载:108/0  |  提交时间:2021/02/03
Influence of coating thickness on the impact damage mode in Fe-based amorphous coatings 期刊论文
SURFACE & COATINGS TECHNOLOGY, 2020, 卷号: 390, 页码: 15
作者:  Guo, H.;  Wu, N. C.;  Zhang, Y. L.;  Zhang, S. D.;  Sun, W. H.;  Wang, J. Q.
收藏  |  浏览/下载:148/0  |  提交时间:2021/02/02
Fe-based amorphous coating  X-ray tomography  Impact damage mechanism  Maximum shear stress  Coating thickness  
Influence of coating thickness on the impact damage mode in Fe-based amorphous coatings 期刊论文
SURFACE & COATINGS TECHNOLOGY, 2020, 卷号: 390, 页码: 15
作者:  Guo, H.;  Wu, N. C.;  Zhang, Y. L.;  Zhang, S. D.;  Sun, W. H.;  Wang, J. Q.
收藏  |  浏览/下载:127/0  |  提交时间:2021/02/02
Fe-based amorphous coating  X-ray tomography  Impact damage mechanism  Maximum shear stress  Coating thickness  
Enhanced bending fatigue resistance of a 50CrMnMoVNb spring steel with decarburized layer by surface spinning strengthening 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2019, 卷号: 124, 页码: 277-287
作者:  Ren, C. X.;  Wang, D. Q. Q.;  Wang, Q.;  Guo, Y. S.;  Zhang, Z. J.;  Shao, C. W.;  Yang, H. J.;  Zhang, Z. F.
收藏  |  浏览/下载:150/0  |  提交时间:2021/02/02
Spring steel  Three-point bending fatigue  Surface decarburization  Surface spinning strengthening (3S)  Fatigue life