Predictions of the full-life pressurised water stress corrosion cracking behaviour of 690 weld joints 期刊论文
JOURNAL OF NUCLEAR MATERIALS, 2025, 卷号: 605, 页码: 13
作者:  Li, Hui;  Li, Gang;  Sun, Wei;  Shao, Xuejiao;  Ma, Guowen;  Ming, Hongliang;  Zhu, Yichao
收藏  |  浏览/下载:4/0  |  提交时间:2025/04/27
Pressurised water stress corrosion cracking  Inconel 690 alloy  690 weld joints  Crack growth rate  Dynamics model  Crack initiation  
Influence of solution treatment on the corrosion fatigue behavior of an as forged Mg-Zn-Y-Zr alloy 期刊论文
INTERNATIONAL JOURNAL OF FATIGUE, 2019, 卷号: 120, 页码: 46-55
作者:  Wang, B. J.;  Xu, D. K.;  Wang, S. D.;  Sheng, L. Y.;  Zeng, Rong-Chang;  Han, En-hou
收藏  |  浏览/下载:131/0  |  提交时间:2021/02/02
Magnesium alloy  Fatigue crack initiation  Corrosion  Corrosion fatigue  Hydrogen embrittlement  
Synergistic Effect of Mo, W, Mn and Cr on the Passivation Behavior of a Fe-Based Amorphous Alloy Coating 期刊论文
ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2018, 卷号: 31, 期号: 3, 页码: 308-320
作者:  Tian, WP;  Yang, HW;  Zhang, SD;  Yang, HW (reprint author), Shenyang Univ Technol, Sch Mat Sci & Engn, Shenyang 110178, Liaoning, Peoples R China.;  Zhang, SD (reprint author), Chinese Acad Sci, Inst Met Res, Shenyang Natl Lab Mat Sci, Shenyang 110016, Liaoning, Peoples R China.
收藏  |  浏览/下载:137/0  |  提交时间:2018/06/05
Bulk Metallic Glasses  Austenitic Stainless-steels  High Corrosion-resistance  Iron-chromium Alloys  Erosion-corrosion  Hard Chromium  Molybdenum  Hcl  Cr3c2-nicr  Initiation  
Recent progress in fatigue behavior of Mg alloys in air and aqueous media: A review 期刊论文
JOURNAL MATER SCI TECHNOL, 2017, 卷号: 33, 期号: 10, 页码: 1075-1086
作者:  Wang, B. J.;  Wang, S. D.;  Xu, D. K.;  Han, E. H.;  Xu, DK (reprint author), Chinese Acad Sci, Inst Met Res, CAS Key Lab Nucl Mat & Safety Assessment, Shenyang 110016, Liaoning, Peoples R China.
收藏  |  浏览/下载:214/0  |  提交时间:2018/01/10
Magnesium Alloys  Fatigue  Corrosion Fatigue  Crack Initiation  Hydrogen Embrittlement  
Effect of corrosion attack on the fatigue behavior of an as-cast Mg-7%Gd-5%Y-1%Nd-0.5%Zr alloy 期刊论文
MATERIALS & DESIGN, 2015, 卷号: 84, 页码: 185-193
作者:  Wang, S. D.;  Xu, D. K.;  Wang, B. J.;  Han, E. H.;  Dong, C.;  dkxu@imr.ac.cn
收藏  |  浏览/下载:101/0  |  提交时间:2016/04/21
Mg Alloy  Corrosion  Cyclic Loading  Fatigue Crack Initiation  Fatigue Behavior  
Effect of pitting nucleation on critical pitting temperature of 316L stainless steel by nitric acid passivation 期刊论文
Corrosion Science, 2015, 卷号: 91, 页码: 232-244
作者:  J.;  Zhang Liu, T.;  Meng, G. Z.;  Shao, Y. W.;  Wang, F. H.
收藏  |  浏览/下载:112/0  |  提交时间:2015/05/08
316l Stainless Steel  Sem  Xps  Pitting Corrosion  Surface-roughness  Chloride Solutions  Corrosion Pits  Resistance  Ion  Inclusions  Dependence  Initiation  Inhibition  
Stress corrosion of pipeline steel under occluded coating disbondment in a red soil environment 期刊论文
Corrosion Science, 2015, 卷号: 93, 页码: 27-38
作者:  M. C.;  Sun Yan, C.;  Xu, J.;  Wu, T. Q.;  Yang, S.;  Ke, W.
收藏  |  浏览/下载:116/0  |  提交时间:2015/05/08
Carbon Steel  Stress Corrosion  Sem  Crevice Corrosion  Scanning Kelvin Probe  Neutral Ph  Cathodic Protection  Crack-growth  Behavior  Electrolyte  Mechanism  Initiation  Beneath  Layer  
Effect of Intermetallic Phases on Corrosion Initiation of AZ91 Alloy With Rare Earth Y Addition 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2015, 卷号: 31, 期号: 5, 页码: 504-511
作者:  Zhang, Li-na;  Jia, Ruiling;  Li, Dan;  Zhang, Wei;  Guo, Feng;  jrl014014@163.com
收藏  |  浏览/下载:113/0  |  提交时间:2016/04/21
Mg Alloy  Yttrium  Intermetallic Phase  Corrosion Initiation  
The reliability of electrochemical noise and current transients characterizing metastable pitting of Al-Mg-Si microelectrodes 期刊论文
Corrosion Science, 2014, 卷号: 80, 页码: 1-6
作者:  L. Guan;  B. Zhang;  J. Q. Wang;  E. H. Han;  W. Ke
收藏  |  浏览/下载:110/0  |  提交时间:2014/03/14
Aluminium  Alloy  Electrochemical Calculation  Afm  Pitting Corrosion  Alkaline Corrosion  Stainless-steel  Aluminum-alloys  Surface-roughness  Corrosion Pits  Nucleation  Growth  Transition  Initiation  Stability  
Simulating corrosion of Al2CuMg phase by measuring ionic currents, chloride concentration and pH 期刊论文
Corrosion Science, 2014, 卷号: 88, 页码: 178-186
作者:  H. W. Shi;  Z. H. Tian;  T. H. Hu;  F. C. Liu;  E. H. Han;  M. Taryba;  S. V. Lamaka
收藏  |  浏览/下载:135/0  |  提交时间:2015/01/14
Intermetallics  Aluminium  Alloy  Sem  Alkaline Corrosion  Aluminum-alloy 2024-t3  Atomic-force Microscopy  Localized Corrosion  Pitting Corrosion  Electrochemical Characteristics  Intermetallic  Phases  Pit Initiation  Aa 2024-t3  S-phase  Aa2024