Synergistic Effect of Mo, W, Mn and Cr on the Passivation Behavior of a Fe-Based Amorphous Alloy Coating 期刊论文
ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2018, 卷号: 31, 期号: 3, 页码: 308-320
作者:  Tian, WP;  Yang, HW;  Zhang, SD;  Yang, HW (reprint author), Shenyang Univ Technol, Sch Mat Sci & Engn, Shenyang 110178, Liaoning, Peoples R China.;  Zhang, SD (reprint author), Chinese Acad Sci, Inst Met Res, Shenyang Natl Lab Mat Sci, Shenyang 110016, Liaoning, Peoples R China.
收藏  |  浏览/下载:137/0  |  提交时间:2018/06/05
Bulk Metallic Glasses  Austenitic Stainless-steels  High Corrosion-resistance  Iron-chromium Alloys  Erosion-corrosion  Hard Chromium  Molybdenum  Hcl  Cr3c2-nicr  Initiation  
Accelerated corrosion of five commercial steels under a ZnCl2-KCl deposit in a reducing environment typical of waste gasification at 673-773 K 期刊论文
Corrosion Science, 2008, 卷号: 50, 期号: 7, 页码: 1900-1906
作者:  W. M. Lu;  T. J. Pan;  K. Zhang;  Y. Niu
Adobe PDF(774Kb)  |  收藏  |  浏览/下载:67/0  |  提交时间:2012/04/13
Steels  Chlorides Salt  Reducing Atmosphere  Corrosion  Atmospheres  Cr  Alloys  Nickel  Hcl  Oxidation  Chlorides  Behavior  Oxygen  Iron  
Corrosion behavior of three iron-based model alloys in reducing atmospheres containing HCl and H2S at 600 degrees C 期刊论文
Corrosion Science, 2007, 卷号: 49, 期号: 3, 页码: 1362-1377
作者:  T. J. Pan;  F. Gesmundo;  Y. Niu
收藏  |  浏览/下载:99/0  |  提交时间:2012/04/13
Fe-cr Alloys  Reducing Atmosphere  Oxidation  Hcl And H2s Effects  High-temperature Corrosion  Fe-cr Alloys  Municipal Incinerators  Hydrogen-chloride  Chromium-alloys  Oxidizing Atmospheres  Fireside  Corrosion  Commercial Steels  Containing Gas  Fired Boilers  
The corrosion of three commercial steels in reducing atmospheres containing HCl and H2S at 873 K 期刊论文
High Temperature Materials and Processes, 2005, 卷号: 24, 期号: 3, 页码: 193-203
作者:  T. J. Pan;  M. Al-Omary;  C. L. Zeng;  W. T. Wu;  Y. Niu
收藏  |  浏览/下载:100/0  |  提交时间:2012/04/14
Fe-cr Steels  Reducing Atmosphere  Corrosion  Hcl And H2s Effects  High-temperature Corrosion  Waste Incineration Environments  Iron-chromium-alloys  Hydrogen-chloride  Gas-mixtures  Oxidizing  Atmospheres  Oxygen Mixtures  Cr Alloys  Fe-cr  Oxidation  
The corrosion behavior of four commercial steels in reducing atmospheres containing HCl at 773-873 K 期刊论文
Oxidation of Metals, 2004, 卷号: 62, 期号: 5-6, 页码: 323-340
作者:  K. Zhang;  Y. Niu;  M. Al-Omary;  W. T. Wu
收藏  |  浏览/下载:150/0  |  提交时间:2012/04/14
Cr Steels Hcl  Reducing Atmosphere  Corrosion  High-temperature Corrosion  Fe-cr Alloys  Hydrogen-chloride  Chromium-alloys  Gas-mixtures  Oxygen  800-degrees-c  Oxidation  Metals  Fuels