Regulating the partially mixed zone via post-weld heat treatment to enhance sulfide stress corrosion cracking resistance of the Inconel 625/X80 weld overlay 期刊论文
MATERIALS TODAY COMMUNICATIONS, 2024, 卷号: 40, 页码: 12
作者:  Zhang, Yan;  Dong, Lijin;  Ma, Cheng;  Zhang, Ziyu;  Wang, Qinying;  Wu, Guiyu;  Liu, Li
收藏  |  浏览/下载:2/0  |  提交时间:2025/04/27
Post-weld heat treatment  Sulfide stress corrosion cracking  Partially mixed zone  Inconel 625/X80 weld overlay  Hydrogen  
Regulating the partially mixed zone via post-weld heat treatment to enhance sulfide stress corrosion cracking resistance of the Inconel 625/X80 weld overlay 期刊论文
MATERIALS TODAY COMMUNICATIONS, 2024, 卷号: 40, 页码: 12
作者:  Zhang, Yan;  Dong, Lijin;  Ma, Cheng;  Zhang, Ziyu;  Wang, Qinying;  Wu, Guiyu;  Liu, Li
收藏  |  浏览/下载:2/0  |  提交时间:2025/04/27
Post-weld heat treatment  Sulfide stress corrosion cracking  Partially mixed zone  Inconel 625/X80 weld overlay  Hydrogen  
Regulating the partially mixed zone via post-weld heat treatment to enhance sulfide stress corrosion cracking resistance of the Inconel 625/X80 weld overlay 期刊论文
MATERIALS TODAY COMMUNICATIONS, 2024, 卷号: 40, 页码: 12
作者:  Zhang, Yan;  Dong, Lijin;  Ma, Cheng;  Zhang, Ziyu;  Wang, Qinying;  Wu, Guiyu;  Liu, Li
收藏  |  浏览/下载:2/0  |  提交时间:2025/04/27
Post-weld heat treatment  Sulfide stress corrosion cracking  Partially mixed zone  Inconel 625/X80 weld overlay  Hydrogen  
Amorphous Phosphorus-Doped Cobalt Sulfide Modified on Silicon Pyramids for Efficient Solar Water Reduction 期刊论文
ACS APPLIED MATERIALS & INTERFACES, 2018, 卷号: 10, 期号: 43, 页码: 37142-37149
作者:  Chen, Chih-Jung;  Liu, Chi-Wei;  Yang, Kai-Chih;  Yin, Li-Chang;  Wei, Da-Hua;  Hu, Shu-Fen;  Liu, Ru-Shi
收藏  |  浏览/下载:130/0  |  提交时间:2021/02/02
water reduction  hydrogen evolution reaction  co-catalyst  P-doped cobalt sulfide  Si pyramids  
Investigation of Interaction Mechanism Between Signaling Molecule Hydrogen Sulfide and L-Lactic Dehydrogenase 期刊论文
CHINESE JOURNAL OF ANALYTICAL CHEMISTRY, 2018, 卷号: 46, 期号: 7, 页码: 1145-1151
作者:  Zhu YanWen;  Liu Ling;  Sun WeiJie;  Yan TingCai;  Tan DeHong;  Zhang Yao;  Bai Bing
收藏  |  浏览/下载:128/0  |  提交时间:2021/02/02
FRESH GARLIC SCALES  H2S  EXPLORATION  OXIDATION  Hydrogen sulfide  L-Lactic dehydrogenase  Cysteine thiols  S-Sulfuration  
Investigation of Interaction Mechanism Between Signaling Molecule Hydrogen Sulfide and L-Lactic Dehydrogenase 期刊论文
CHINESE JOURNAL OF ANALYTICAL CHEMISTRY, 2018, 卷号: 46, 期号: 7, 页码: 1145-1151
作者:  Zhu YanWen;  Liu Ling;  Sun WeiJie;  Yan TingCai;  Tan DeHong;  Zhang Yao;  Bai Bing
收藏  |  浏览/下载:132/0  |  提交时间:2021/02/02
FRESH GARLIC SCALES  H2S  EXPLORATION  OXIDATION  Hydrogen sulfide  L-Lactic dehydrogenase  Cysteine thiols  S-Sulfuration  
HIC and SSC Behavior of High-Strength Pipeline Steels 期刊论文
ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2015, 卷号: 28, 期号: 7, 页码: 799-808
作者:  Shi, Xian-Bo;  Yan, Wei;  Wang, Wei;  Zhao, Lian-Yu;  Shan, Yi-Yin;  Yang, Ke;  kyang@imr.ac.cn
收藏  |  浏览/下载:157/0  |  提交时间:2016/04/21
Hydrogen-induced Cracking  Sulfide Stress Corrosion Cracking  High-strength Pipeline Steel  Martensite/austenite Island (M/a)  
Corrosion Behavior of X52 Anti-H2S Pipeline Steel Exposed to High H2S Concentration Solutions at 90 degrees C 期刊论文
Journal of Materials Science & Technology, 2014, 卷号: 30, 期号: 5, 页码: 504-510
作者:  M. Liu;  J. Q. Wang;  W. Ke;  E. H. Han
收藏  |  浏览/下载:135/0  |  提交时间:2014/07/03
H2s Corrosion  X52 Anti-h2s Pipeline Steel  High Temperature  Iron  Sulfide  Hydrogen-sulfide  Iron  Morphology  Diagrams  
Highly Efficient Deposition Method of Platinum over CdS for H-2 Evolution under Visible Light 期刊论文
Journal of Physical Chemistry C, 2014, 卷号: 118, 期号: 38, 页码: 21928-21934
作者:  G. Xin;  B. Yu;  Y. J. Xia;  T. Hu;  L. M. Liu;  C. F. Li
收藏  |  浏览/下载:127/0  |  提交时间:2015/01/14
Photocatalytic H-2-production Performance  Hydrogen-production  Cadmium-sulfide  Water  Irradiation  Semiconductor  Nanocomposites  Luminescence  Cocatalyst  Oxynitride  
Corrosion behaviour of X52 pipeline steel in high H2S concentration solutions at temperatures ranging from 25 degrees C to 140 degrees C 期刊论文
Corrosion Engineering Science and Technology, 2013, 卷号: 48, 期号: 5, 页码: 380-387
作者:  M. Liu;  J. Wang;  W. Ke
收藏  |  浏览/下载:88/0  |  提交时间:2013/12/24
X52 Pipeline Steel  H2s Corrosion  High Temperature  Corrosion Products  Iron-sulfide Films  Hydrogen-sulfide  Solubility  Autoclaves  Morphology  Pressures  Diagrams  Media  Water