IMR OpenIR

浏览/检索结果: 共10条,第1-10条 帮助

已选(0)清除 条数/页:   排序方式:
Comparative study of microstructure and properties of low-alloy-steel/nickel-based-alloy interfaces in dissimilar metal weld joints prepared by different GTAW methods 期刊论文
MATERIALS CHARACTERIZATION, 2018, 卷号: 139, 页码: 186-196
作者:  Ming, HL;  Wang, JQ;  Han, EH;  Wang, JQ (reprint author), Chinese Acad Sci, Inst Met Res, Liaoning Key Lab Safety & Assessment Tech Nucl Ma, Key Lab Nucl Mat & Safety Assessment, Shenyang 110016, Peoples R China.
收藏  |  浏览/下载:112/0  |  提交时间:2018/06/05
Local Mechanical-properties  Dip Cracking Susceptibility  Stress-corrosion Cracking  Fusion Boundary Region  Safe-end  Ferritic Steel  Part 1  
Microstructure and Local Properties of a Domestic Safe-End Dissimilar Metal Weld Joint by Using Hot-Wire GTAW 期刊论文
ACTA METALLURGICA SINICA, 2017, 卷号: 53, 期号: 1, 页码: 57-69
作者:  Ming Hongliang;  Zhang Zhiming;  Wang Jianqiu;  Han En-Hou;  Su Mingxing
收藏  |  浏览/下载:135/0  |  提交时间:2021/02/02
dissimilar metal weld joint  microstructure  local mechanical property  stress corrosion cracking susceptibility  residual strain  
Microstructure and Local Properties of a Domestic Safe-End Dissimilar Metal Weld Joint by Using Hot-Wire GTAW 期刊论文
ACTA METALLURGICA SINICA, 2017, 卷号: 53, 期号: 1, 页码: 57-69
作者:  Ming Hongliang;  Zhang Zhiming;  Wang Jianqiu;  Han En-Hou;  Su Mingxing
收藏  |  浏览/下载:97/0  |  提交时间:2021/02/02
dissimilar metal weld joint  microstructure  local mechanical property  stress corrosion cracking susceptibility  residual strain  
Microstructure, local mechanical properties and stress corrosion cracking susceptibility of an SA508-52M-316LN safe-end dissimilar metal weld joint by GTAW 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 卷号: 669, 页码: 279-290
作者:  Ming, Hongliang;  Zhu, Ruolin;  Zhang, Zhiming;  Wang, Jianqiu;  Han, En. -Hou;  Ke, Wei;  Su, Mingxing;  Wang, JQ (reprint author), Chinese Acad Sci, Inst Met Res, Liaoning KeyLab Safety & Assessment Tech Nucl Mat, Key Lab Nucl Mat & Safety Assessment, Shenyang 110016, Peoples R China.
收藏  |  浏览/下载:111/0  |  提交时间:2016/08/22
Dissimilar Metal Welded Joint  Microstructure  Residual Strain  Local Mechanical Properties  Local Stress Corrosion Cracking Susceptibility  
Characterization of low alloy ferritic steel-Ni base alloy dissimilar metal weld interface by SPM techniques, SEM/EDS, TEM/EDS and SVET 期刊论文
Materials Characterization, 2015, 卷号: 100, 页码: 50-60
作者:  S. Y.;  Ding Wang, J.;  Ming, H. L.;  Zhang, Z. M.;  Wang, J. Q.
收藏  |  浏览/下载:118/0  |  提交时间:2015/05/08
Weld  Interface  Spm  Tem  Sem  Svet  Duplex Stainless-steel  Probe Force Microscopy  Stress-corrosion  Cracking  Local Mechanical-properties  Fusion Boundary Region  Phase  Particles  Al-alloys  Joint  Skpfm  Microstructure  
Influence of Organic Inhibitors on the Corrosion Behavior of Steel Rebar inside Mortar Specimens Immersed in Saturated NaCl Solution 期刊论文
Acta Physico-Chimica Sinica, 2010, 卷号: 26, 期号: 9, 页码: 2354-2360
作者:  L. G. Zheng;  H. Y. Yang
收藏  |  浏览/下载:98/0  |  提交时间:2012/04/13
Corrosion Inhibitor  Protection Of Steel Rebar  Local Corrosion Induced  By Cl(-)  Electrochemical Technique  Chloride-induced Corrosion  Passive Film Breakdown  Borate Buffer  Solution  Reinforced-concrete  Time  System  Media  Iron  Eis  
Designed oscillations of the Fe/H(2)SO(4) system with the flow injection in a partially-closed environment 期刊论文
Electrochemistry Communications, 2009, 卷号: 11, 期号: 10, 页码: 1888-1891
作者:  M. Zeng;  C. Wang;  L. Li
Adobe PDF(265Kb)  |  收藏  |  浏览/下载:71/0  |  提交时间:2012/04/13
Partially-closed Environment  Flow Injection  Local Perturbation  Artificial Oscillations  Sulfuric-acid-solution  Potentiostatic Current Oscillations  Active  Transition-state  Solution Interfaces  Digital Holography  Pitting  Corrosion  Iron  Electrodissolution  Perturbation  
Stress corrosion cracking of X-70 pipeline steel in near neutral pH solution subjected to constant toad and cyclic toad testing 期刊论文
Corrosion Engineering Science and Technology, 2007, 卷号: 42, 期号: 2, 页码: 123-129
作者:  B. Y. Fang;  E. H. Han;  J. Q. Wang;  W. Ke
收藏  |  浏览/下载:75/0  |  提交时间:2012/04/13
Stress Corrosion Cracking  Pipeline Steel  Constant Loading  Cyclic  Loading  Near Neutral Ph Solution  Local Strain Rate  Strain-rate  Transport Processes  Creep  X-80  
Influence of strain rate on near-neutral pH environmentally assisted cracking of pipeline steels 期刊论文
ACTA METALLURGICA SINICA, 2005, 卷号: 41, 期号: 11, 页码: 1174-1182
作者:  Fang, BY;  Han, EH;  Wang, JQ;  Ke, W
收藏  |  浏览/下载:140/0  |  提交时间:2021/02/02
local strain rate  stress corrosion cracking  corrosion fatigue  strain assisted corrosion cracking  environmentally assisted cracking  
Experimental studies on the local corrosion of low alloy steels in 3.5% NaCl 期刊论文
Corrosion Science, 2001, 卷号: 43, 期号: 3, 页码: 397-411
作者:  Y. Gan;  Y. Li;  H. C. Lin
收藏  |  浏览/下载:142/0  |  提交时间:2012/04/14
Low Alloy Steel  Local Corrosion  Occluded Corrosion Cavity  Simulated  Cell  Chloride