IMR OpenIR

浏览/检索结果: 共5条,第1-5条 帮助

已选(0)清除 条数/页:   排序方式:
The effect of Si additions on the high temperature oxidation of a ternary Ni-10Cr-4Al alloy in 1 atm O(2) at 1100 degrees C 期刊论文
Corrosion Science, 2009, 卷号: 51, 期号: 3, 页码: 511-517
作者:  S. Wang;  Y. Wu;  C. S. Ni;  Y. Niu
Adobe PDF(560Kb)  |  收藏  |  浏览/下载:62/0  |  提交时间:2012/04/13
Alloy  Nickel  Oxidation  Most-reactive Components  Internal Oxidation  External Oxidation  Oxidant Pressures  Transition  
Accelerated corrosion of Fe-xCr-10Al alloys containing 0-20 at.% Cr induced by sulfur and chlorine in a reducing atmosphere at 600 degrees C 期刊论文
Oxidation of Metals, 2008, 卷号: 69, 期号: 1-2, 页码: 63-76
作者:  W. M. Lu;  T. J. Pan;  Y. Niu
Adobe PDF(496Kb)  |  收藏  |  浏览/下载:73/0  |  提交时间:2012/04/13
Fe-xcr-10al  Oxidation  Chlorine And Sulfur Effect  High-oxidant Pressures  Al-y Alloys  High-temperature Corrosion  Most-reactive Components  Internal Oxidation  Hydrogen-chloride  External Oxidation  Ternary Alloys  Iron  Oxygen  
The nature of the third-element effect in the oxidation of Fe-xCr-3 at.% Al alloys in 1 atm O-2 at 1000 degrees C 期刊论文
Corrosion Science, 2008, 卷号: 50, 期号: 2, 页码: 345-356
作者:  Y. Niu;  S. Wang;  F. Gao;  Z. G. Zhang;  F. Gesmundo
Adobe PDF(748Kb)  |  收藏  |  浏览/下载:71/0  |  提交时间:2012/04/13
Fe-al Alloys  Oxidation  Chromium Effect  High-temperature Oxidation  High-oxidant Pressures  Iron-aluminum-alloys  Fe-cr-al  Most-reactive Components  Internal  Oxidation  External Oxidation  Ternary Alloys  Gamma-iron  y Alloys  
The effect of Si additions on the high-temperature oxidation of a ternary Ni-10Cr-4Al alloy in 1 ATM O(2) AT 900-1000 degrees C 期刊论文
Oxidation of Metals, 2008, 卷号: 69, 期号: 5-6, 页码: 299-315
作者:  S. Wang;  Y. Wu;  F. Gesmundo;  Y. Niu
Adobe PDF(942Kb)  |  收藏  |  浏览/下载:91/0  |  提交时间:2012/04/13
Ni-cr-si-al Alloys  Oxidation  Third-element Effect  Intermediate Oxidant Pressures  Most-reactive Components  1200 Degrees  c  Internal Oxidation  External Oxidation  Transition  At.percent  Silicon  X=0  
Internal attack of Fe-xCr-10Al alloys induced by the presence of chlorine and sulfur in a reducing atmosphere at 973 K 期刊论文
Scripta Materialia, 2007, 卷号: 57, 期号: 2, 页码: 97-100
作者:  T. J. Pan;  Y. Niu
收藏  |  浏览/下载:77/0  |  提交时间:2012/04/13
Fe-xcr-10al Alloys  Internal Attack  Cl And s Effect  Most-reactive Components  High-oxidant Pressures  High-temperature  Corrosion Behavior  External Oxidation  Ternary Alloys  Iron  Chloridation  Transition  Chromium