| Complete Kinetic Maps for Binary Alloys Forming Two Insoluble Oxides Under High Oxygen Pressures 期刊论文 Oxidation of Metals, 2010, 卷号: 73, 期号: 1-2, 页码: 65-81 作者: F. Gesmundo; S. Wang; Y. Niu
Adobe PDF(455Kb)  |   收藏  |  浏览/下载:151/0  |  提交时间:2012/04/13 Binary Alloys Oxidation Maps High Oxidant Pressures Internal Oxidation External Oxidation Copper Legierungen Transition Oxydation Scale Bei |
| An Improved Treatment of the Kinetics of Coupled Internal Oxidation by a Single Oxidant of the Two Most-Reactive Components of Ternary Alloys and of the Conditions for the Transition to Their External Oxidation 期刊论文 Oxidation of Metals, 2009, 卷号: 72, 期号: 5-6, 页码: 279-297 作者: S. Wang; F. Gesmundo; Y. Niu
Adobe PDF(1296Kb)  |   收藏  |  浏览/下载:75/0  |  提交时间:2012/04/13 Ternary Alloys Internal Oxidation Low Oxidant Pressures High Oxidant Pressures |
| Effect of Zn Additions on the Oxidation of Cu-2 at.% Al and Cu-4 at.% Al Alloys in 1 atm O(2) at 800 A degrees C 期刊论文 Oxidation of Metals, 2009, 卷号: 71, 期号: 1-2, 页码: 43-61 作者: F. Gao; F. Gesmundo; Y. Niu
Adobe PDF(613Kb)  |   收藏  |  浏览/下载:85/0  |  提交时间:2012/04/13 Third-element Effect Oxidation Cu-zn-al Alloys Most-reactive Component Intermediate Oxidant Pressures Alpha-solid-solutions External Oxidation Ternary Alloys Internal Oxidation Transition Copper Diffusion Kinetics |
| The effect of Si additions on the high temperature oxidation of a ternary Ni-10Cr-4Al alloy in 1 atm O(2) at 1100 degrees C 期刊论文 Corrosion Science, 2009, 卷号: 51, 期号: 3, 页码: 511-517 作者: S. Wang; Y. Wu; C. S. Ni; Y. Niu
Adobe PDF(560Kb)  |   收藏  |  浏览/下载:63/0  |  提交时间:2012/04/13 Alloy Nickel Oxidation Most-reactive Components Internal Oxidation External Oxidation Oxidant Pressures Transition |
| Accelerated corrosion of Fe-xCr-10Al alloys containing 0-20 at.% Cr induced by sulfur and chlorine in a reducing atmosphere at 600 degrees C 期刊论文 Oxidation of Metals, 2008, 卷号: 69, 期号: 1-2, 页码: 63-76 作者: W. M. Lu; T. J. Pan; Y. Niu
Adobe PDF(496Kb)  |   收藏  |  浏览/下载:75/0  |  提交时间:2012/04/13 Fe-xcr-10al Oxidation Chlorine And Sulfur Effect High-oxidant Pressures Al-y Alloys High-temperature Corrosion Most-reactive Components Internal Oxidation Hydrogen-chloride External Oxidation Ternary Alloys Iron Oxygen |
| The nature of the third-element effect in the oxidation of Fe-xCr-3 at.% Al alloys in 1 atm O-2 at 1000 degrees C 期刊论文 Corrosion Science, 2008, 卷号: 50, 期号: 2, 页码: 345-356 作者: Y. Niu; S. Wang; F. Gao; Z. G. Zhang; F. Gesmundo
Adobe PDF(748Kb)  |   收藏  |  浏览/下载:73/0  |  提交时间:2012/04/13 Fe-al Alloys Oxidation Chromium Effect High-temperature Oxidation High-oxidant Pressures Iron-aluminum-alloys Fe-cr-al Most-reactive Components Internal Oxidation External Oxidation Ternary Alloys Gamma-iron y Alloys |
| The effect of Si additions on the high-temperature oxidation of a ternary Ni-10Cr-4Al alloy in 1 ATM O(2) AT 900-1000 degrees C 期刊论文 Oxidation of Metals, 2008, 卷号: 69, 期号: 5-6, 页码: 299-315 作者: S. Wang; Y. Wu; F. Gesmundo; Y. Niu
Adobe PDF(942Kb)  |   收藏  |  浏览/下载:95/0  |  提交时间:2012/04/13 Ni-cr-si-al Alloys Oxidation Third-element Effect Intermediate Oxidant Pressures Most-reactive Components 1200 Degrees c Internal Oxidation External Oxidation Transition At.percent Silicon X=0 |
| High temperature scaling of Ni-xSi-10 at.% A1 alloys in 1 atm of pure O-2 期刊论文 Corrosion Science, 2007, 卷号: 49, 期号: 3, 页码: 1656-1672 作者: Y. Wu; Y. Niu
 收藏  |  浏览/下载:101/0  |  提交时间:2012/04/13 Ternary Ni-xsi-10al Alloys Oxidation Silicon Effect Al-si Alloys 2-phase Binary-alloys Internal Oxidation Ni-al External Scale Ternary Alloys Oxidant Pressures Aluminum Alloys Degrees c 1 Atm |
| Internal attack of Fe-xCr-10Al alloys induced by the presence of chlorine and sulfur in a reducing atmosphere at 973 K 期刊论文 Scripta Materialia, 2007, 卷号: 57, 期号: 2, 页码: 97-100 作者: T. J. Pan; Y. Niu
 收藏  |  浏览/下载:79/0  |  提交时间:2012/04/13 Fe-xcr-10al Alloys Internal Attack Cl And s Effect Most-reactive Components High-oxidant Pressures High-temperature Corrosion Behavior External Oxidation Ternary Alloys Iron Chloridation Transition Chromium |
| Criteria for the formation of protective Al2O3 scales on Fe-Al and Fe-Cr-Al alloys 期刊论文 Corrosion Science, 2006, 卷号: 48, 期号: 3, 页码: 741-765 作者: Z. G. Zhang; F. Gesmundo; P. Y. Hou; Y. Niu
 收藏  |  浏览/下载:75/0  |  提交时间:2012/05/18 Fecral Ternary Alloys Oxidation Cr Effect Iron-aluminum-alloys High-temperature Oxidation High Oxidant Pressures y Alloys Internal Oxidation Growth Mechanisms External Oxidation Self-diffusion Base Alloys Gamma-iron |