IMR OpenIR

浏览/检索结果: 共6条,第1-6条 帮助

已选(0)清除 条数/页:   排序方式:
Accelerated corrosion of five commercial steels under a ZnCl2-KCl deposit in a reducing environment typical of waste gasification at 673-773 K 期刊论文
Corrosion Science, 2008, 卷号: 50, 期号: 7, 页码: 1900-1906
作者:  W. M. Lu;  T. J. Pan;  K. Zhang;  Y. Niu
Adobe PDF(774Kb)  |  收藏  |  浏览/下载:65/0  |  提交时间:2012/04/13
Steels  Chlorides Salt  Reducing Atmosphere  Corrosion  Atmospheres  Cr  Alloys  Nickel  Hcl  Oxidation  Chlorides  Behavior  Oxygen  Iron  
Corrosion behavior of three iron-based model alloys in reducing atmospheres containing HCl and H2S at 600 degrees C 期刊论文
Corrosion Science, 2007, 卷号: 49, 期号: 3, 页码: 1362-1377
作者:  T. J. Pan;  F. Gesmundo;  Y. Niu
收藏  |  浏览/下载:96/0  |  提交时间:2012/04/13
Fe-cr Alloys  Reducing Atmosphere  Oxidation  Hcl And H2s Effects  High-temperature Corrosion  Fe-cr Alloys  Municipal Incinerators  Hydrogen-chloride  Chromium-alloys  Oxidizing Atmospheres  Fireside  Corrosion  Commercial Steels  Containing Gas  Fired Boilers  
Corrosion of three commercial steels under ZnCl2-KCl deposits in a reducing atmosphere containing HCl and H2S at 400-500 degrees C 期刊论文
Oxidation of Metals, Oxidation of Metals, 2007, 2007, 卷号: 67, 67, 期号: 1-2, 页码: 107-127, 107-127
作者:  T. J. Pan;  C. L. Zeng;  Y. Niu
收藏  |  浏览/下载:89/0  |  提交时间:2012/04/13
Steels  Steels  Chlorides  Chlorides  Reducing Atmosphere  Reducing Atmosphere  Corrosion  Corrosion  Hcl And H2s Effects  Hcl And H2s Effects  High-temperature Corrosion  High-temperature Corrosion  Alloys  Alloys  Oxidation  Oxidation  Mixtures  Mixtures  Nickel  Nickel  Iron  Iron  400-700-degrees-c  400-700-degrees-c  Environments  Environments  Chloridation  Chloridation  Chromium  Chromium  
The corrosion of three commercial steels in reducing atmospheres containing HCl and H2S at 873 K 期刊论文
High Temperature Materials and Processes, 2005, 卷号: 24, 期号: 3, 页码: 193-203
作者:  T. J. Pan;  M. Al-Omary;  C. L. Zeng;  W. T. Wu;  Y. Niu
收藏  |  浏览/下载:99/0  |  提交时间:2012/04/14
Fe-cr Steels  Reducing Atmosphere  Corrosion  Hcl And H2s Effects  High-temperature Corrosion  Waste Incineration Environments  Iron-chromium-alloys  Hydrogen-chloride  Gas-mixtures  Oxidizing  Atmospheres  Oxygen Mixtures  Cr Alloys  Fe-cr  Oxidation  
The corrosion behavior of four commercial steels in reducing atmospheres containing HCl at 773-873 K 期刊论文
Oxidation of Metals, 2004, 卷号: 62, 期号: 5-6, 页码: 323-340
作者:  K. Zhang;  Y. Niu;  M. Al-Omary;  W. T. Wu
收藏  |  浏览/下载:140/0  |  提交时间:2012/04/14
Cr Steels Hcl  Reducing Atmosphere  Corrosion  High-temperature Corrosion  Fe-cr Alloys  Hydrogen-chloride  Chromium-alloys  Gas-mixtures  Oxygen  800-degrees-c  Oxidation  Metals  Fuels  
High temperature corrosion behavior of steel 2.25CrMo in reducing atmosphere containing chlorine 期刊论文
ACTA METALLURGICA SINICA, 2003, 卷号: 39, 期号: 5, 页码: 541-543
作者:  Zhang, K;  Niu, Y;  Wu, WT
收藏  |  浏览/下载:83/0  |  提交时间:2021/02/02
steel 2.25CrMo  reducing atmosphere containing chlorine  high temperature corrosion  waste gasification