IMR OpenIR

浏览/检索结果: 共11条,第1-10条 帮助

已选(0)清除 条数/页:   排序方式:
Low cycle fatigue behavior and microstructure evolution of a fourth-generation single crystal superalloy at 800 °C 期刊论文
MATERIALS CHARACTERIZATION, 2023, 卷号: 205, 页码: 14
作者:  Liang, Z. Y.;  Tan, Z. H.;  Zhang, C. H.;  Zhang, S.;  Tao, X. P.;  Wang, X. G.;  Jafri, S. M. Abbas;  Shi, Z. W.;  Yang, Y. H.;  Liu, J. D.;  Liu, J. L.;  Li, J. G.;  Zhou, Y. Z.;  Sun, X. F.
收藏  |  浏览/下载:8/0  |  提交时间:2024/01/07
Fourth-generation Ni-base single crystal super-alloy  Low cycle fatigue  Cyclic hardening  Dislocation configuration  Deformation mechanism  
Investigation on microstructure and mechanical properties of a vacuum brazed joint of gamma '-strengthened Co-based single crystal superalloy before and after the post-bond heat treatment 期刊论文
VACUUM, 2020, 卷号: 177, 页码: 11
作者:  Wang, S. Y.;  Sun, Y.;  Hou, X. Y.;  Cui, C. Y.;  Sun, X. F.;  Zhou, Y. Z.
收藏  |  浏览/下载:139/0  |  提交时间:2021/02/02
Transient liquid phase bonding  gamma '-strengthened Co-Based single crystal super alloy  Microstructure  Microhardness  
Effects of grain size on the high-cycle fatigue behavior of IN792 superalloy 期刊论文
Materials & Design, 2015, 卷号: 65, 页码: 57-64
作者:  B. N. Du;  J. X. Yang;  C. Y. Cui;  X. F. Sun
收藏  |  浏览/下载:134/0  |  提交时间:2015/01/14
Nickel Super Alloy  Grain Refinement  High Cycle Fatigue  Nickel-base Superalloy  Elevated-temperatures  Crack-growth  Mechanical-properties  Tensile Properties  Microstructure  Initiation  Deformation  Character  713lc  
Experimental and Numerical Research on Deformation Behavior of Thin-Walled and Large Expansion Ratio Guide Vane Liner in Hydroforming Process 期刊论文
哈尔滨工业大学学报:英文版, 2015, 卷号: 22.0, 期号: 004, 页码: 1-9
作者:  Cheng Pengzhi;  Lang Lihui;  Ge Yulong;  Ruan Shangwen;  Duan Xinmin;  Shao Tianwei
收藏  |  浏览/下载:120/0  |  提交时间:2021/02/26
tube hydroforming  super alloy  ultra-thin-wall  large expansion ratio  useful wrinkle  plastic buckling  critical buckling stress  
Research on super-hydrophobic surface of biodegradable magnesium alloys used for vascular stents 期刊论文
Materials Science & Engineering C-Materials for Biological Applications, 2013, 卷号: 33, 期号: 5, 页码: 2885-2890
作者:  P. Wan;  J. Y. Wu;  L. L. Tan;  B. C. Zhang;  K. Yang
收藏  |  浏览/下载:105/0  |  提交时间:2013/12/24
Magnesium Alloy  Super-hydrophobic  Corrosion  Hemocompatibility  Superhydrophobic Surfaces  Platelet-adhesion  Stearic-acid  Fabrication  
CRYSTAL MORPHOLOGIES AND THE PHASES IN THE Mg-6Zn-3Y ALLOY SOLIDIFIED UNDER SUPER-HIGH PRESSURE 期刊论文
ACTA METALLURGICA SINICA, 2011, 卷号: 47, 期号: 12, 页码: 1550-1554
作者:  Lin Xiaoping;  Dong Yun;  Xu Rui;  Sun Guifang;  Jia Shihui
收藏  |  浏览/下载:115/0  |  提交时间:2021/02/02
MICROSTRUCTURE  Mg-6Zn-3Y alloy  super-high pressure solidification  dendritic crystal  cellular crystal  phase component  
Super-hydrophobic surface on pure magnesium substrate by wet chemical method 期刊论文
Applied Surface Science, 2010, 卷号: 256, 期号: 12, 页码: 3837-3840
作者:  Y. H. Wang;  W. Wang;  L. Zhong;  J. Wang;  Q. L. Jiang;  X. Y. Guo
Adobe PDF(600Kb)  |  收藏  |  浏览/下载:157/0  |  提交时间:2012/04/13
Magnesium  Super-hydrophobic  Wet Chemical Method  Stearic Acid  Superhydrophobic Surfaces  Fabrication  Alloy  
Effect of gamma ' formation and strengthening elements on microstructures and stress rupture property of single crystal super-alloys 期刊论文
China Foundry, 2010, 卷号: 7, 期号: 3, 页码: 265-269
作者:  L. R. Liu;  H. J. Chen;  T. Jin;  X. F. Sun;  H. Guan;  Z. Q. Hu
收藏  |  浏览/下载:74/0  |  提交时间:2012/04/13
Gamma ' Phase  Microstructures  Stress Rupture Property  Single Crystal  Super-alloy  Creep-behavior  Superalloys  
Role of Re and Co on microstructures and gamma ' coarsening in single crystal superalloys 期刊论文
Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2008, 卷号: 479, 期号: 1-2, 页码: 148-156
作者:  W. Z. Wang;  T. Jin;  J. L. Liu;  X. F. Sun;  H. R. Guan;  Z. Q. Hu
Adobe PDF(2451Kb)  |  收藏  |  浏览/下载:92/0  |  提交时间:2012/04/13
Rhenium  Cobalt  Gamma' Coarsening  Tcp Phase  Single Crystal Superalloy  Base Super-alloy  Cobalt  Additions  Mar-m247  Tantalum  Tungsten  Phase  
The crack initiation mechanism of the forged Mg-Zn-Y-Zr alloy in the super-long fatigue life regime 期刊论文
Scripta Materialia, 2007, 卷号: 56, 期号: 1, 页码: 40912
作者:  D. K. Xu;  L. Liu;  Y. B. Xu;  E. H. Han
收藏  |  浏览/下载:68/0  |  提交时间:2012/04/13
Magnesium Alloy  Fatigue Strength  Fatigue Limit  Super-long Fatigue  Life  Az31 Magnesium Alloy  Cycle Fatigue  Cast Magnesium  Fracture  Steels  Deformation  Behavior  Failure  Limit