IMR OpenIR

浏览/检索结果: 共10条,第1-10条 帮助

限定条件    
已选(0)清除 条数/页:   排序方式:
Microstructural evolution and its influence on the wear resistance of a laser directed energy deposited Ni-based single crystal superalloy 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2025, 卷号: 205, 页码: 127-138
作者:  Ren, Chenyu;  Chen, Kai;  Liang, Jingjing;  Narayan, R. Lakshmi;  Ramamurty, Upadrasta;  Li, Jinguo
收藏  |  浏览/下载:5/0  |  提交时间:2025/04/27
In-situ formed gradient nanostructure  Enhanced wear resistance  Laser-directed energy deposition additive  manufacturing  Ni-based single crystal superalloys  Plastic deformation  
Generation mechanism and motion behavior of sliver defect in single crystal Ni-based superalloy 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2023, 卷号: 137, 页码: 232-246
作者:  Xia, Huxiang;  Yang, Yanhong;  Feng, Qiushui;  Xu, Qingyan;  Dong, Hongbiao;  Liu, Baicheng
收藏  |  浏览/下载:64/0  |  提交时间:2023/05/09
Single crystal Ni-based superalloys  Directional solidification  Sliver defect  Phase -field simulation  
Generation mechanism and motion behavior of sliver defect in single crystal Ni-based superalloy 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2023, 卷号: 137, 页码: 232-246
作者:  Xia, Huxiang;  Yang, Yanhong;  Feng, Qiushui;  Xu, Qingyan;  Dong, Hongbiao;  Liu, Baicheng
收藏  |  浏览/下载:39/0  |  提交时间:2023/05/09
Single crystal Ni-based superalloys  Directional solidification  Sliver defect  Phase -field simulation  
Effect of thermal exposure on the microstructure and creep properties of a fourth-generation Ni-based single crystal superalloy 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 卷号: 69, 页码: 180-187
作者:  Huang, Yeshun;  Wang, Xinguang;  Cui, Chuanyong;  Tan, Zihao;  Li, Jinguo;  Yang, Yanhong;  Liu, Jinlai;  Zhou, Yizhou;  Sun, Xiaofeng
收藏  |  浏览/下载:129/0  |  提交时间:2021/10/15
Ni-based single crystal superalloys  Thermal exposure  Microstructural evolution  Creep properties  Porosity  
Effect of thermal exposure on the microstructure and creep properties of a fourth-generation Ni-based single crystal superalloy 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 卷号: 69, 页码: 180-187
作者:  Huang, Yeshun;  Wang, Xinguang;  Cui, Chuanyong;  Tan, Zihao;  Li, Jinguo;  Yang, Yanhong;  Liu, Jinlai;  Zhou, Yizhou;  Sun, Xiaofeng
收藏  |  浏览/下载:133/0  |  提交时间:2021/10/15
Ni-based single crystal superalloys  Thermal exposure  Microstructural evolution  Creep properties  Porosity  
Microstructure and composition evolution of a single-crystal superalloy caused by elements interdiffusion with an overlay NiCrAlY coating on oxidation 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2020, 卷号: 45, 页码: 49-58
作者:  Yang, Lanlan;  Chen, Minghui;  Wang, Jinlong;  Qiao, Yanxin;  Guo, Pingyi;  Zhu, Shenglong;  Wang, Fuhui
收藏  |  浏览/下载:111/0  |  提交时间:2021/02/02
Single-crystal superalloys  NiCrAlY coating  High-temperature oxidation  Arc ion plating  Elements interdiffusion  Microstructure  
Microstructure and composition evolution of a single-crystal superalloy caused by elements interdiffusion with an overlay NiCrAlY coating on oxidation 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2020, 卷号: 45, 页码: 49-58
作者:  Yang, Lanlan;  Chen, Minghui;  Wang, Jinlong;  Qiao, Yanxin;  Guo, Pingyi;  Zhu, Shenglong;  Wang, Fuhui
收藏  |  浏览/下载:130/0  |  提交时间:2021/02/02
Single-crystal superalloys  NiCrAlY coating  High-temperature oxidation  Arc ion plating  Elements interdiffusion  Microstructure  
Effects of Al on microstructural stability and related stress-rupture properties of a third-generation single crystal superalloy 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2019, 卷号: 35, 期号: 11, 页码: 2537-2542
作者:  Sun, Jingxia;  Liu, Jinlai;  Liu, Lirong;  Zhou, Yizhou;  Li, Jinguo;  Sun, Xiaofeng
收藏  |  浏览/下载:146/0  |  提交时间:2021/02/02
Ni base single crystal superalloys  Thermal exposure  Microstructural stability  Stress-rupture property  Al  
Influences of Re on low-cycle fatigue behaviors of single crystal superalloys at intermediate temperature 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2019, 卷号: 35, 期号: 9, 页码: 1917-1924
作者:  Liu, Liu;  Meng, Jie;  Liu, Jinlai;  Zou, Mingke;  Zhang, Haifeng;  Sun, Xudong;  Zhou, Yizhou
收藏  |  浏览/下载:129/0  |  提交时间:2021/02/02
Single crystal superalloys  Low-cycle fatigue  Deformation behaviors  Deformation mechanisms  
Influences of Re on low-cycle fatigue behaviors of single crystal superalloys at intermediate temperature 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2019, 卷号: 35, 期号: 9, 页码: 1917-1924
作者:  Liu, Liu;  Meng, Jie;  Liu, Jinlai;  Zou, Mingke;  Zhang, Haifeng;  Sun, Xudong;  Zhou, Yizhou
收藏  |  浏览/下载:129/0  |  提交时间:2021/02/02
Single crystal superalloys  Low-cycle fatigue  Deformation behaviors  Deformation mechanisms