Influence of Ta/Al ratio on the microstructure and creep property of a Ru-containing Ni-based single-crystal superalloy 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 卷号: 89, 页码: 16-23
Authors:  Song, Wei;  Wang, Xinguang;  Li, Jinguo;  Meng, Jie;  Yang, Yanhong;  Liu, Jinlai;  Liu, Jide;  Zhou, Yizhou;  Sun, Xiaofeng
Favorite  |  View/Download:9/0  |  Submit date:2021/11/22
Ni-based superalloys  Ta/Al ratio  High temperature creep  Interfacial dislocation networks  gamma-rafting  
Effect of Pt-Al bond coat on the high-cycle fatigue behaviour of a second-generation single crystal nickel-based superalloy at different temperatures 期刊论文
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2021, 卷号: 14, 页码: 567-581
Authors:  Tao, X. P.;  Wang, X. G.;  Zhou, Y. Z.;  Tan, K. J.;  Meng, J.;  Liang, J. J.;  Yang, Y. H.;  Liu, J. L.;  Liu, J. D.;  Li, J. G.;  Sun, X. F.
Favorite  |  View/Download:6/0  |  Submit date:2021/11/22
High-cycle fatigue  Pt-Al bond coat  Ni-based superalloy  Fracture behaviour  Deformation mechanism  
A new refractory Ni7Nb2 phase identified in Laves eutectic regions by TEM study 期刊论文
ACTA MATERIALIA, 2021, 卷号: 214, 页码: 10
Authors:  Ge, Hualong;  Xing, Weiwei;  Chen, Bo;  Hu, Xiaobing;  Zheng, Shijian;  Liu, Kui;  Ma, Xiuliang
Favorite  |  View/Download:5/0  |  Submit date:2021/10/15
Nickel-based superalloys  Inconel 718  In-situ transmission electron microscopy  Laves phase  Eutectic  Ni-Nb phase  
Quantifying the Influences of Carbides and Porosities on the Fatigue Crack Evolution of a Ni-Based Single-Crystal Superalloy using X-ray Tomography 期刊论文
ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2021, 页码: 13
Authors:  Liu, Keli;  Wang, Junsheng;  Wang, Bing;  Mao, Pengcheng;  Yang, Yanhong;  Zhou, Yizhou
Favorite  |  View/Download:3/0  |  Submit date:2021/10/15
X-ray tomography  Ni-based superalloys  Fatigue  Porosity  Carbide  Crack initiation  Crack propagation  
Effect of substituting Mo for W on gamma/gamma ' partitioning behaviors of alloying elements in heat-treated second generation Ni based single crystal superalloys: An atom probe tomography study 期刊论文
INTERMETALLICS, 2021, 卷号: 134, 页码: 9
Authors:  Ai, Cheng;  Li, Qing;  Zhang, Jun;  Su, Haijun;  Yang, Wenchao;  Liu, Lin;  Ru, Yi;  Zhang, Heng;  Song, Yuanyuan;  Chen, Yongnan;  Li, Shusuo;  Gong, Shengkai
Favorite  |  View/Download:3/0  |  Submit date:2021/10/15
Ni based single crystal superalloy  Substituting Mo for W  Atom probe tomography (APT)  gamma/gamma ' partitioning behaviors of alloying elements  
A correlative multidimensional study of gamma ' precipitates with Ta addition in Re-containing Ni-based single crystal superalloys 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 卷号: 75, 页码: 68-77
Authors:  Zhang, Jiachen;  Huang, Taiwen;  Cao, Kaili;  Chen, Jia;  Zong, Huajing;  Wang, Dong;  Zhang, Jian;  Zhang, Jun;  Liu, Lin
Favorite  |  View/Download:8/0  |  Submit date:2021/10/15
Tantalum  Ni-based superalloys  Atom probe tomography  Lattice misfit  Coarsening kinetics  
Investigating the evolution of freckles into sliver defects in Ni-based single-crystal superalloy castings 期刊论文
MATERIALS TODAY COMMUNICATIONS, 2021, 卷号: 27, 页码: 14
Authors:  Han, Dongyu;  Jiang, Weiguo;  Xiao, Jiuhan;  Li, Kaiwen;  Lu, Yuzhang;  Lou, Langhong
Favorite  |  View/Download:8/0  |  Submit date:2021/10/15
Ni-based superalloys  Directional solidification  Freckle evolution  Slivers  
Influence of Pt-Al Coating on Hot Corrosion Resistance Behaviors of a Ni-Based Single-Crystal Superalloy 期刊论文
ACTA METALLURGICA SINICA, 2021, 卷号: 57, 期号: 6, 页码: 780-790
Authors:  Wang Di;  Wang Dong;  Xie Guang;  Wang Li;  Dong Jiasheng;  Chen Lijia
Favorite  |  View/Download:9/0  |  Submit date:2021/10/15
Pt-Al coating  hot corrosion  single-crystal superalloy  Ni-based alloy  
An in-situ formed ceramic/alloy/ceramic sandwich barrier to resist elements interdiffusion between NiCrAlY coating and a Ni-based superalloy 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 卷号: 70, 页码: 1-11
Authors:  Guo, Cean;  Zhou, Feng;  Chen, Minghui;  Wang, Jinlong;  Zhu, Shenglong;  Wang, Fuhui
Favorite  |  View/Download:4/0  |  Submit date:2021/10/15
Superalloys  NiCrAlY  coating  High-temperature oxidation  Elements interdiffusion  Diffusion barrier  
An in-situ formed ceramic/alloy/ceramic sandwich barrier to resist elements interdiffusion between NiCrAlY coating and a Ni-based superalloy 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 卷号: 70, 页码: 1-11
Authors:  Guo, Cean;  Zhou, Feng;  Chen, Minghui;  Wang, Jinlong;  Zhu, Shenglong;  Wang, Fuhui
Favorite  |  View/Download:4/0  |  Submit date:2021/10/15
Superalloys  NiCrAlY  coating  High-temperature oxidation  Elements interdiffusion  Diffusion barrier