Effect of Hf on microstructure and creep properties of a hot corrosion resistant nickel-based single crystal superalloy 期刊论文
CHINA FOUNDRY, 2025, 页码: 9
作者:  Ma, Li;  Wang, Dong;  Zhang, Gong;  Shen, Jian;  Zhang, Jian
收藏  |  浏览/下载:6/0  |  提交时间:2025/04/27
Ni-based single crystal superalloys  hafnium  creep properties  MC carbides  hot corrosion resistance  
Microstructural evolution and its influence on the wear resistance of a laser directed energy deposited Ni-based single crystal superalloy 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2025, 卷号: 205, 页码: 127-138
作者:  Ren, Chenyu;  Chen, Kai;  Liang, Jingjing;  Narayan, R. Lakshmi;  Ramamurty, Upadrasta;  Li, Jinguo
收藏  |  浏览/下载:5/0  |  提交时间:2025/04/27
In-situ formed gradient nanostructure  Enhanced wear resistance  Laser-directed energy deposition additive  manufacturing  Ni-based single crystal superalloys  Plastic deformation  
Effect of withdrawal rate on the microstructure and static recrystallization behavior of Ni-based single crystal superalloy 期刊论文
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 卷号: 33, 页码: 8252-8264
作者:  Xu, F. Z.;  Xiong, W.;  Lin, Y. C.;  Ma, D. X.;  Cheng, B. W.;  Xie, G.;  He, D. G.;  Zhao, Y. X.;  Li, L.;  Deng, Y. P.
收藏  |  浏览/下载:4/0  |  提交时间:2025/04/27
Single-crystal superalloys  Recrystallization  Directional solidification  Withdrawal rate  Microstructure  
Effect of withdrawal rate on the microstructure and static recrystallization behavior of Ni-based single crystal superalloy 期刊论文
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 卷号: 33, 页码: 8252-8264
作者:  Xu, F. Z.;  Xiong, W.;  Lin, Y. C.;  Ma, D. X.;  Cheng, B. W.;  Xie, G.;  He, D. G.;  Zhao, Y. X.;  Li, L.;  Deng, Y. P.
收藏  |  浏览/下载:3/0  |  提交时间:2025/04/27
Single-crystal superalloys  Recrystallization  Directional solidification  Withdrawal rate  Microstructure  
Enhanced fatigue performance of γ/γ′ dual-phase single-crystal superalloys with graded surface nanostructures 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 卷号: 916, 页码: 16
作者:  Dang, Xiaofeng;  Liang, Xiaoqing;  He, Weifeng;  Lu, Kaiju;  Li, Jinguo;  Zhou, Liucheng;  Wang, Xin;  Luo, Sihai;  Li, Yao
收藏  |  浏览/下载:4/0  |  提交时间:2025/04/27
Ni-based single-crystal superalloys  Shot peening  Fatigue life  Graded surface nanostructures  gamma/gamma ' dual-phase architecture  
Enhanced fatigue performance of γ/γ′ dual-phase single-crystal superalloys with graded surface nanostructures 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 卷号: 916, 页码: 16
作者:  Dang, Xiaofeng;  Liang, Xiaoqing;  He, Weifeng;  Lu, Kaiju;  Li, Jinguo;  Zhou, Liucheng;  Wang, Xin;  Luo, Sihai;  Li, Yao
收藏  |  浏览/下载:3/0  |  提交时间:2025/04/27
Ni-based single-crystal superalloys  Shot peening  Fatigue life  Graded surface nanostructures  gamma/gamma ' dual-phase architecture  
Duration-affected creep behaviors of Ni-based single crystal superalloys with/without rhenium addition designed for IGT application 期刊论文
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 卷号: 864, 页码: 13
作者:  Lu, Fan;  Lu, Song;  Antonov, Stoichko;  Li, Longfei;  He, Siliang;  Hou, Muchun;  Wang, Dong;  Zhang, Jian;  Feng, Qiang
收藏  |  浏览/下载:10/0  |  提交时间:2024/01/07
Ni-based single crystal superalloys  Duration effect  Microstructural evolution  Deformation mechanism  Re effect  
Effect of solution heat treatment on creep properties of a nickel-based single crystal superalloy 期刊论文
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2021, 卷号: 15, 页码: 4702-4713
作者:  Yunling, Du;  Yang, Yanhong;  Diao, Aimin;  Li, Yongmei;  Wang, Xinguang;  Zhou, Yizhou;  Li, Jinguo;  Sun, Xiaofeng
收藏  |  浏览/下载:193/0  |  提交时间:2022/01/27
Nickel-based single crystal superalloys  Microstructural evolution  Creep behavior  Solution heat-treatment  
Effect of thermal exposure on the microstructure and creep properties of a fourth-generation Ni-based single crystal superalloy 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 卷号: 69, 页码: 180-187
作者:  Huang, Yeshun;  Wang, Xinguang;  Cui, Chuanyong;  Tan, Zihao;  Li, Jinguo;  Yang, Yanhong;  Liu, Jinlai;  Zhou, Yizhou;  Sun, Xiaofeng
收藏  |  浏览/下载:129/0  |  提交时间:2021/10/15
Ni-based single crystal superalloys  Thermal exposure  Microstructural evolution  Creep properties  Porosity  
Effect of thermal exposure on the microstructure and creep properties of a fourth-generation Ni-based single crystal superalloy 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 卷号: 69, 页码: 180-187
作者:  Huang, Yeshun;  Wang, Xinguang;  Cui, Chuanyong;  Tan, Zihao;  Li, Jinguo;  Yang, Yanhong;  Liu, Jinlai;  Zhou, Yizhou;  Sun, Xiaofeng
收藏  |  浏览/下载:133/0  |  提交时间:2021/10/15
Ni-based single crystal superalloys  Thermal exposure  Microstructural evolution  Creep properties  Porosity