Achieving excellent elevated-temperature mechanical properties in dual-phase high-entropy alloys via nanoscale co-precipitation and heterostructure engineering 期刊论文
ACTA MATERIALIA, 2025, 卷号: 284, 页码: 18
作者:  Niu, M. C.;  Qiu, S.;  Yu, Q.;  Li, W.;  Zhang, S. Z.;  Guo, J. M.;  Luan, J. H.;  Wang, W.;  Yang, T.;  Wang, X. L.;  Jiao, Z. B.
收藏  |  浏览/下载:2/0  |  提交时间:2025/04/27
Eutectic high-entropy alloy  Microstructure formation mechanism  Precipitation  High-temperature mechanical properties  Strengthening mechanism  
Effects of laser energy density on the resistance to wear and cavitation erosion of FeCrNiMnAl high entropy alloy coatings by laser cladding 期刊论文
MATERIALS CHEMISTRY AND PHYSICS, 2025, 卷号: 329, 页码: 17
作者:  Yu, D. T.;  Wang, R.;  Wu, C. L.;  Wang, Z. Z.;  Zhang, S.;  Zhang, C. H.;  Chen, H. T.;  Tao, X. P.
收藏  |  浏览/下载:4/0  |  提交时间:2025/04/27
Laser cladding  High entropy alloy  Wear  Cavitation erosion  
In vivo biodegradation and biological properties of a Mg-Zn-Ca amorphous alloy for bone defect repair 期刊论文
MATERIALS TECHNOLOGY, 2024, 卷号: 39, 期号: 1, 页码: 19
作者:  Meng, J.;  Zhang, Y.;  Yu, X.;  Jiao, J.;  Tan, L.;  Yu, B.
收藏  |  浏览/下载:1/0  |  提交时间:2025/04/27
Mg-Zn-Ca amorphous alloy  bone defects  biodegradation  osteogenesis  
Wear, corrosion and cavitation erosion behavior of WC-reinforced FeCrNiMnAl ceramic-high entropy alloy composite coatings by laser cladding 期刊论文
CERAMICS INTERNATIONAL, 2024, 卷号: 50, 期号: 24, 页码: 55790-55800
作者:  Yu, D. T.;  Wang, R.;  Wu, C. L.;  Wang, Z. . Z.;  Zhao, X. B.;  Zhang, S.;  Zhang, C. . H.;  Tao, X. P.
收藏  |  浏览/下载:3/0  |  提交时间:2025/04/27
Laser cladding  High entropy alloy  Wear  Cavitation erosion  
Iso-Material Manufactured 17-4PH Stainless Steel to Enhance the Nano-indentation, Corrosion, and Cavitation Erosion Behavior 期刊论文
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 页码: 16
作者:  Yu, D. T.;  Wang, R.;  Wu, C. L.;  Zhang, S.;  Zhang, C. H.;  Chen, H. T.;  Tao, X. P.
收藏  |  浏览/下载:1/0  |  提交时间:2025/04/27
cavitation erosion  corrosion  iso-material manufacturing  laser surface melting  nano-indentation  
Effects of heat treatment on the nano-indentation, corrosion and cavitation erosion behavior of 17-4PH stainless steel by laser surface melting 期刊论文
SURFACE & COATINGS TECHNOLOGY, 2024, 卷号: 484, 页码: 14
作者:  Yu, D. T.;  Wu, C. L.;  Zhang, S.;  Zhang, C. H.;  Chen, H. T.;  Tao, X. P.
收藏  |  浏览/下载:2/0  |  提交时间:2025/04/27
Laser surface melting  Heat treatment  Nano-indentation  Corrosion  Cavitation erosion  
Magnetism and magnetocaloric effects in tetragonal structure of RE5Ni2Sb (R = Er, Ho) compounds 期刊论文
JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2024, 卷号: 594, 页码: 5
作者:  Yu, S. L.;  Tian, L.;  Wang, J. F.;  Zhao, X. G.;  Li, D.;  Mo, Z. J.;  Li, B.
收藏  |  浏览/下载:2/0  |  提交时间:2025/04/27
Magnetism  Magnetocaloric effects  Tetragonal structure  Magnetic phase transition  RE 5 Ni 2 Sb compounds  
Effect of abrasive water jet peening on NaCl-induced hot corrosion behavior of Ti-6Al-4V 期刊论文
VACUUM, 2023, 卷号: 210, 页码: 10
作者:  Chakkravarthy, V.;  Oliveira, J. P.;  Mahomed, Anisa;  Yu, Nan;  Manojkumar, P.;  Lakshmanan, M.;  Zhang, Long;  Raja, V.;  Jerome, S.;  Prabhu, T. Ram;  Narayan, R. L.
收藏  |  浏览/下载:47/0  |  提交时间:2023/05/09
Hot corrosion  Abrasive cavitation peening  Ti-6Al-4V alloy  NaCl molten Salt  Compressive residual stress  
γ' 相对高钨镍基高温合金拉伸和持久变形行为的影响 期刊论文
材料研究学报, 2023, 卷号: 37, 期号: 1, 页码: 29-38
作者:  韦林;  周思耕;  盛乃成;  于金江;  侯桂臣;  王标;  权佳;  周亦胄;  孙晓峰;  康涌
收藏  |  浏览/下载:82/0  |  提交时间:2024/01/08
metallic materials  K416B alloy  γ' precipitation  tensile behavior  duration  dislocation  金属材料  K416B合金  γ'析出相  拉伸  持久  位错  
深水压力-流速交互作用下Al-Zn-In牺牲阳极的自腐蚀行为研究 期刊论文
中国腐蚀与防护学报, 2023, 卷号: 43, 期号: 2, 页码: 329-336
作者:  张睿;  崔宇;  刘莉;  王福会
收藏  |  浏览/下载:10/0  |  提交时间:2024/01/08
hydrostatic pressure  flow  sacrificial anode  self-corrosion  深水压力  流速  牺牲阳极  自腐蚀