IMR OpenIR

浏览/检索结果: 共251条,第1-10条 帮助

已选(0)清除 条数/页:   排序方式:
Unifie d mixe d conductivity model 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2025, 卷号: 213, 页码: 80-89
作者:  Li, X. T.;  Zhang, Z. J.;  Dai, R. J.;  Liu, R.;  Qu, Z.;  Wang, S. G.;  Li, H. T.;  Hu, W. J.;  Wang, Q. Z.;  Ma, Z. Y.;  Zhang, Z. F.
收藏  |  浏览/下载:7/0  |  提交时间:2025/04/27
Composite materials  Conductivity  Elastic modulus  Permeability coefficient  Diffusion coefficient  Multiphase interpenetrating structure  
Coercivity mechanism and microstructure evolution of perpendicular magnetic anisotropic Nd-Fe-B thick films annealed by pulsed laser 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 卷号: 1020, 页码: 8
作者:  Liu, S.;  Zhao, X. T.;  Liu, L.;  Liu, W.;  Li, C. H.;  Ma, J.;  Li, D.;  Zhang, Z. D.
收藏  |  浏览/下载:4/0  |  提交时间:2025/04/27
Nd-Fe-B thick film  Laser annealing  Perpendicular magnetic anisotropy  Coercivity mechanism  
Tensile properties and damage mechanisms of 3D printed Ti-24Nb-4Zr-8Sn alloy and polyurea interpenetrating phase composites 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 卷号: 1007, 页码: 8
作者:  Lu, C. Q.;  Li, S. J.;  Liu, Z. Q.;  Liu, D. R.;  Zhao, T.;  Gong, D. L.;  Hou, W. T.;  Yang, R.;  Hao, Y. L.
收藏  |  浏览/下载:2/0  |  提交时间:2025/04/27
Interpenetrating phase composites  Polyurea  Additive manufacturing  Tensile properties  Hysteresis loss energy  
Tensile properties and damage mechanisms of 3D printed Ti-24Nb-4Zr-8Sn alloy and polyurea interpenetrating phase composites 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 卷号: 1007, 页码: 8
作者:  Lu, C. Q.;  Li, S. J.;  Liu, Z. Q.;  Liu, D. R.;  Zhao, T.;  Gong, D. L.;  Hou, W. T.;  Yang, R.;  Hao, Y. L.
收藏  |  浏览/下载:3/0  |  提交时间:2025/04/27
Interpenetrating phase composites  Polyurea  Additive manufacturing  Tensile properties  Hysteresis loss energy  
Cause analysis of the cracking at the gas outlet edge of a gas turbine combustor 期刊论文
PRAKTISCHE METALLOGRAPHIE-PRACTICAL METALLOGRAPHY, 2024, 卷号: 61, 期号: 6, 页码: 398-410
作者:  Zhang, H.;  Zhang, G.;  Zhao, T.;  Liu, L.;  Dong, C.;  Qu, S.;  Zhang, Z.
收藏  |  浏览/下载:3/0  |  提交时间:2025/04/27
Gas turbine combustor  K648 superalloy  thermal fatigue cracking  Gasturbinenbrennkammer  Superlegierung K648  thermische Erm & uuml  dungsrisse  
A study of shot peening and spinning rolling on fatigue of Al 7075 alloy samples 期刊论文
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2024, 页码: 9
作者:  Guan, Y.;  Zhang, Z. J.;  Gong, B. S.;  Wang, H. W.;  Shao, C. W.;  Liu, R.;  Hou, J. P.;  Li, X. T.;  Zhao, Z. K.;  Sheinerman, A. G.;  Zhang, Z. F.
收藏  |  浏览/下载:3/0  |  提交时间:2025/04/27
Al alloy  fatigue life  hardness  residual stress  spinning rolling  
A study of shot peening and spinning rolling on fatigue of Al 7075 alloy samples 期刊论文
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2024, 页码: 9
作者:  Guan, Y.;  Zhang, Z. J.;  Gong, B. S.;  Wang, H. W.;  Shao, C. W.;  Liu, R.;  Hou, J. P.;  Li, X. T.;  Zhao, Z. K.;  Sheinerman, A. G.;  Zhang, Z. F.
收藏  |  浏览/下载:2/0  |  提交时间:2025/04/27
Al alloy  fatigue life  hardness  residual stress  spinning rolling  
A study of shot peening and spinning rolling on fatigue of Al 7075 alloy samples 期刊论文
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2024, 页码: 9
作者:  Guan, Y.;  Zhang, Z. J.;  Gong, B. S.;  Wang, H. W.;  Shao, C. W.;  Liu, R.;  Hou, J. P.;  Li, X. T.;  Zhao, Z. K.;  Sheinerman, A. G.;  Zhang, Z. F.
收藏  |  浏览/下载:4/0  |  提交时间:2025/04/27
Al alloy  fatigue life  hardness  residual stress  spinning rolling  
Pt-modification on the thermal cycling behavior of NiCoCrAlYTa coating: A case study 期刊论文
CORROSION SCIENCE, 2024, 卷号: 230, 页码: 15
作者:  Li, Y. Y.;  Zhang, C.;  Ji, H. Z.;  Jiang, Y. M.;  Liu, T. Y.;  Li, S.;  Bao, Z. B.;  Xu, N.;  Zhu, S. L.;  Wang, F. H.
收藏  |  浏览/下载:1/0  |  提交时间:2025/04/27
NiCoCrAlYTa  Thermal cycling  High velocity oxygen fuel (HVOF)  Residual stress  Microstructure  
Influence of Ta plus Al on the microstructure evolution of two Ru-containing Ni-based single crystal superalloys deposited with γ′ plus β NiAl coating at extremely high temperature 期刊论文
SURFACE & COATINGS TECHNOLOGY, 2023, 卷号: 472, 页码: 11
作者:  Ge, M. T.;  Li, Y. M.;  Tan, Z. H.;  Tao, X. P.;  Yang, Y. H.;  Liu, J. D.;  Liu, J. L.;  Zou, M. K.;  Zhang, C. H.;  Zhang, S.;  Wang, X. G.;  Li, J. G.;  Zhou, Y. Z.;  Sun, X. F.
收藏  |  浏览/下载:21/0  |  提交时间:2024/01/08
Ru-containing SX superalloys  NiAl coating  Microstructural evolution  Recrystallization  Secondary reaction zone (SRZ)  Ta plus Al