The internal oxidation of ternary alloys. VIII: The transition from the internal to the external oxidation of the two most-reactive components under high-oxidant pressures 期刊论文
Oxidation of Metals, 2006, 卷号: 65, 期号: 5-6, 页码: 329-355
作者:  Y. Niu;  F. Gesmundo
收藏  |  浏览/下载:76/0  |  提交时间:2012/04/14
Ternary Alloys  Transition To The External Oxidation  High-oxidant  Pressures  2-phase Binary-alloys  Cr-al Alloys  High-temperature Oxidation  Forming  Insoluble Oxides  Possible Scaling Modes  Fe-cu Alloys  Air Oxidation  Approximate Analysis  H-2-h2s Mixtures  Diffusion  
Oxidation of two ternary Fe-Cu-5Al alloys in 1 x 10(5) Pa pure oxygen at 700 degrees C 期刊论文
Transactions of Nonferrous Metals Society of China, 2006, 卷号: 16, 页码: S829-S833
作者:  J. H. Xiang;  Y. Niu;  W. T. Wu;  G. D. Liu
收藏  |  浏览/下载:156/0  |  提交时间:2012/04/14
Fe-cu-5al  Ternary Alloy  High Temperature Oxidation  At.percent-al-alloys  Forming Insoluble Oxides  Approximate Analysis  External Oxidation  Oxidant Pressures  Degrees-c  1 Atm  O-2  800-900-degrees-c  1-atm  
Oxidation behavior of ternary Fe-15Cu-5Al and Fe-85Cu-5Al alloys in pure oxygen at 900 degrees C 期刊论文
Transactions of Nonferrous Metals Society of China, 2006, 卷号: 16, 页码: S2038-S2041
作者:  J. H. Xiang;  Y. Niu;  X. Z. Duan
收藏  |  浏览/下载:84/0  |  提交时间:2012/04/14
Fe-15cu-5al Alloy  Fe-85cu-5al Alloy  Ternary Alloy  Oxidation Behavior  At.percent-al-alloys  Forming Insoluble Oxides  External Oxidation  1  Atm  Approximate Analysis  Oxidant Pressures  Air Oxidation  O-2  800-900-degrees-c  
The oxidation of two ternary Fe-Cu-10 at.% Al alloys in 1 atm of pure O-2 at 800-900 degrees C 期刊论文
Corrosion Science, 2005, 卷号: 47, 期号: 6, 页码: 1493-1505
作者:  J. H. Xiang;  Y. Niu;  F. Gesmundo
收藏  |  浏览/下载:94/0  |  提交时间:2012/04/14
Ternary Alloys  Iron-copper Base  Oxidation  Aluminum Effect  Cu-cr Alloys  Forming Insoluble Oxides  2-phase Binary-alloys  Low  Oxidant Pressures  Internal Oxidation  External Oxidation  Air  Oxidation  Approximate Analysis  Ag Alloys  700-900-degrees-c  
The oxidation of two ternary Ni-Cu-10 at.% Al alloys in 1 atm of pure O-2 at 800-900 degrees C 期刊论文
Corrosion Science, 2004, 卷号: 46, 期号: 8, 页码: 2025-2039
作者:  J. H. Xiang;  F. Gesmundo;  Y. Niu
收藏  |  浏览/下载:81/0  |  提交时间:2012/04/14
Ternary Alloys  Nickel-copper Base  Oxidation  Aluminium Effect  Forming Insoluble Oxides  Approximate Analysis  External Oxidation  Oxidant Pressures  Aluminum-alloys  Scale  Nickel  Microstructure  Growth  
Oxidation of two ternary Fe-Cu-5 at.% al alloys in 1 atm of pure O-2 at 800 degrees C 期刊论文
Oxidation of Metals, 2004, 卷号: 61, 期号: 5-6, 页码: 403-421
作者:  J. H. Xiang;  Y. Niu;  F. Gesmundo
收藏  |  浏览/下载:102/0  |  提交时间:2012/04/14
Ternary Alloys  Iron-copper Base  Oxidation  Aluminium Effect  Low Oxidant Pressures  Cu-cr Alloys  Forming Insoluble Oxides  2-phase  Binary-alloys  Internal Oxidation  External Oxidation  Air Oxidation  Approximate Analysis  H-2-h2s Mixtures  Ag Alloys  
Phase stability, kinetic diagrams and diffusion path in high temperature oxidation of binary solid-solution alloys 期刊论文
Journal of Materials Science & Technology, 2003, 卷号: 19, 期号: 6, 页码: 545-552
作者:  Y. Niu;  F. Gesmundo
收藏  |  浏览/下载:88/0  |  提交时间:2012/04/14
Binary Alloys  Oxidation  Thermodynamic And Kinetic Diagrams  Diffusion  Path  Low Oxidant Pressures  Forming Insoluble Oxides  Most-reactive  Component  Possible Scaling Modes  Internal Oxidation  Stable Oxide  Approximate Analysis  Activity-coefficient  External Oxidation  Dilute  Solutions  
Use of the phase stability and kinetic diagrams in relation to the high temperature oxidation of binary solid-solution alloys 期刊论文
Intermetallics, 2003, 卷号: 11, 期号: 11-12, 页码: 1361-1367
作者:  Y. Niu;  F. Gesmundo;  G. Cacciamani
收藏  |  浏览/下载:76/0  |  提交时间:2012/04/14
Oxidation  Thermodynamic And Thermochemical Properties  High Oxidant Pressures  Forming Insoluble Oxides  Possible Scaling  Modes  Most-stable Oxide  Internal Oxidation  Approximate Analysis  External Oxidation  Scales  Corrosion  Metals