IMR OpenIR

浏览/检索结果: 共12条,第1-10条 帮助

已选(0)清除 条数/页:   排序方式:
IrO2-SiO2 binary oxide films: Preparation, physiochemical characterization and their electrochemical properties 期刊论文
ELECTROCHIMICA ACTA, 2010, 卷号: 55, 期号: 15, 页码: 4587-4593
作者:  Wang, Xiao-Mei;  Hu, Ji-Ming;  Zhang, Jian-Qing
收藏  |  浏览/下载:94/0  |  提交时间:2021/02/02
IrO2  SiO2  Binary oxide  Electrocatalyst  Oxygen evolution reaction (OER)  
Theoretical elastic stiffness, structural stability and thermal conductivity of La(2)T(2)O(7) (T = Ge, Ti, Sn, Zr, Hf) pyrochlore 期刊论文
Acta Materialia, 2010, 卷号: 58, 期号: 13, 页码: 4369-4377
作者:  B. Liu;  J. Y. Wang;  F. Z. Li;  Y. C. Zhou
Adobe PDF(886Kb)  |  收藏  |  浏览/下载:109/0  |  提交时间:2012/04/13
Non-binary Oxides  Mechanical Properties  Thermal Conductivity  Density  Functional Theory  Local Density Approximations (Lda)  Oxide Pyrochlores  a(2)b(2)o(7)  Simulation  Disorder  
IrO(2)-SiO(2) binary oxide films: Preparation, physiochemical characterization and their electrochemical properties 期刊论文
Electrochimica Acta, 2010, 卷号: 55, 期号: 15, 页码: 4587-4593
作者:  X. M. Wang;  J. M. Hu;  J. Q. Zhang
Adobe PDF(877Kb)  |  收藏  |  浏览/下载:94/0  |  提交时间:2012/04/13
Iro(2)  Sio(2)  Binary Oxide  Electrocatalyst  Oxygen Evolution Reaction  (Oer)  X-ray-diffraction  Surface Characterization  Oxygen Evolution  Thin-films  Electrodes  Titanium  Electrocatalysts  Iridium  Anodes  Acid  
Bioaccumulation of heavy metals by Phragmites australis cultivated in synthesized substrates 期刊论文
JOURNAL OF ENVIRONMENTAL SCIENCES, 2009, 卷号: 21, 期号: 10, 页码: 1409-1414
作者:  Wang He;  Jia Yongfeng
收藏  |  浏览/下载:85/0  |  提交时间:2021/02/02
BINARY OXIDE SUSPENSIONS  TRIN. EX STEUDEL  MINE TAILINGS  IRON PLAQUE  ACCUMULATION  ADSORPTION  FE  SEDIMENTS  CADMIUM  WETLAND  heavy metals  bioaccumulation  metal oxides  adsorption  
Phase stability, kinetic diagrams and diffusion path in high temperature oxidation of binary solid-solution alloys 期刊论文
Journal of Materials Science & Technology, 2003, 卷号: 19, 期号: 6, 页码: 545-552
作者:  Y. Niu;  F. Gesmundo
收藏  |  浏览/下载:91/0  |  提交时间:2012/04/14
Binary Alloys  Oxidation  Thermodynamic And Kinetic Diagrams  Diffusion  Path  Low Oxidant Pressures  Forming Insoluble Oxides  Most-reactive  Component  Possible Scaling Modes  Internal Oxidation  Stable Oxide  Approximate Analysis  Activity-coefficient  External Oxidation  Dilute  Solutions  
Oxidation of a three-phase Cu-45Ni-30Cr alloy at 700-800 degrees C under 1 atm O-2 期刊论文
Oxidation of Metals, 2002, 卷号: 57, 期号: 5-6, 页码: 395-407
作者:  Z. Q. Cao;  F. Gesmundo;  M. Al-Omary;  Y. Niu
收藏  |  浏览/下载:85/0  |  提交时间:2012/04/14
Cu-ni-cr  Multiphase Alloy  High Temperatures  Oxidation  2-phase Binary-alloys  Low-oxygen Pressures  High-temperature Oxidation  Most-reactive Component  Possible Scaling Modes  High Oxidant Pressures  Cu-cr Alloys  Air Oxidation  Internal Oxidation  Stable Oxide  
Grain size effects on the oxidation of two-phase Cu-Fe alloys 期刊论文
Corrosion Science, 2002, 卷号: 44, 期号: 7, 页码: 1457-1468
作者:  Y. S. Li;  Y. Niu;  F. Gesmundo;  F. H. Wang
收藏  |  浏览/下载:53/0  |  提交时间:2012/04/14
Oxidation  Fe-cu Alloys  Nanophase Materials  2-phase Binary-alloys  High-temperature Oxidation  Most-reactive  Component  High Oxidant Pressures  Possible Scaling Modes  Air  Oxidation  Selective Oxidation  Internal Oxidation  Stable Oxide  Cr  Alloys  
Oxidation of two ternary Cu-Ni-20 wt.% Cr alloys at 700-800 degrees C in 1 atm O-2 期刊论文
Oxidation of Metals, 2001, 卷号: 56, 期号: 3-4, 页码: 287-297
作者:  Z. Q. Cao;  Y. Niu;  F. Gesmundo
收藏  |  浏览/下载:102/0  |  提交时间:2012/04/14
Copper  Nickel  Chromium  Alloys  Oxidation  2-phase Binary-alloys  High-temperature Oxidation  Most-reactive  Component  Possible Scaling Modes  High Oxidant Pressures  Fe-cu Alloys  Air Oxidation  Internal Oxidation  Stable Oxide  Corrosion  
Oxidation of the three-phase alloy Cu-20Ni-20Cr AT 973-1073 K in 101 kPa O-2 期刊论文
High Temperature Materials and Processes, 2001, 卷号: 20, 期号: 5-6, 页码: 377-383
作者:  Z. Q. Cao;  Y. Niu;  G. Farne;  F. Gesmundo
收藏  |  浏览/下载:78/0  |  提交时间:2012/04/14
Cu-ni-cr  Multiphase Alloy  High Temperatures  Oxidation  2-phase Binary-alloys  High-temperature Oxidation  Most-reactive  Component  Possible Scaling Modes  High Oxidant Pressures  Fe-cu Alloys  Air Oxidation  Internal Oxidation  Stable Oxide  Cr Alloys  
The air oxidation of two-phase Co-Cu alloys at 600-800 degrees C 期刊论文
Corrosion Science, Corrosion Science, Corrosion Science, 2000, 2000, 2000, 卷号: 42, 42, 42, 期号: 5, 页码: 799-815, 799-815, 799-815
作者:  Y. Niu;  J. Song;  F. Gesmundo;  G. Farne;  G. Fu;  C. Zeng
收藏  |  浏览/下载:141/0  |  提交时间:2012/04/14
Cobalt  Cobalt  Cobalt  Copper  Copper  Copper  Two-phase Alloys  Two-phase Alloys  Two-phase Alloys  Oxidation  Oxidation  Oxidation  2-phase Binary-alloys  2-phase Binary-alloys  2-phase Binary-alloys  High-temperature Oxidation  High-temperature Oxidation  High-temperature Oxidation  Most-reactive  Most-reactive  Most-reactive  Component  Component  Component  High Oxidant Pressures  High Oxidant Pressures  High Oxidant Pressures  Possible Scaling Modes  Possible Scaling Modes  Possible Scaling Modes  Low-oxygen  Low-oxygen  Low-oxygen  Pressures  Pressures  Pressures  Internal Oxidation  Internal Oxidation  Internal Oxidation  Stable Oxide  Stable Oxide  Stable Oxide  Cr Alloys  Cr Alloys  Cr Alloys  700-900-degrees-c  700-900-degrees-c  700-900-degrees-c