Internal attack of Fe-xCr-10Al alloys induced by the presence of chlorine and sulfur in a reducing atmosphere at 973 K 期刊论文
Scripta Materialia, 2007, 卷号: 57, 期号: 2, 页码: 97-100
作者:  T. J. Pan;  Y. Niu
收藏  |  浏览/下载:77/0  |  提交时间:2012/04/13
Fe-xcr-10al Alloys  Internal Attack  Cl And s Effect  Most-reactive Components  High-oxidant Pressures  High-temperature  Corrosion Behavior  External Oxidation  Ternary Alloys  Iron  Chloridation  Transition  Chromium  
Corrosion of three commercial steels under ZnCl2-KCl deposits in a reducing atmosphere containing HCl and H2S at 400-500 degrees C 期刊论文
Oxidation of Metals, Oxidation of Metals, 2007, 2007, 卷号: 67, 67, 期号: 1-2, 页码: 107-127, 107-127
作者:  T. J. Pan;  C. L. Zeng;  Y. Niu
收藏  |  浏览/下载:87/0  |  提交时间:2012/04/13
Steels  Steels  Chlorides  Chlorides  Reducing Atmosphere  Reducing Atmosphere  Corrosion  Corrosion  Hcl And H2s Effects  Hcl And H2s Effects  High-temperature Corrosion  High-temperature Corrosion  Alloys  Alloys  Oxidation  Oxidation  Mixtures  Mixtures  Nickel  Nickel  Iron  Iron  400-700-degrees-c  400-700-degrees-c  Environments  Environments  Chloridation  Chloridation  Chromium  Chromium  
Corrosion of iron and four commercial steels in a Cl-containing oxidizing atmosphere at 500 similar to 600 degrees C 期刊论文
Journal of Materials Science & Technology, 2004, 卷号: 20, 期号: 2, 页码: 213-216
作者:  K. Zhang;  Y. Niu;  C. L. Zeng;  W. T. Wu
收藏  |  浏览/下载:86/0  |  提交时间:2012/04/14
Commercial Steels  High Temperature  Chlorination  Waste Incineration  Fe-cr Alloys  High-temperature  Chloridation  Oxidation