IMR OpenIR

浏览/检索结果: 共14条,第1-10条 帮助

已选(0)清除 条数/页:   排序方式:
High-Temperature Oxidation Behavior of SIMP Steel at 800 A degrees C 期刊论文
OXIDATION OF METALS, 2018, 卷号: 89, 期号: 43102, 页码: 49-60
作者:  Shi, QQ;  Zhang, LL;  Yan, W;  Wang, W;  Yin, PH;  Shan, YY;  Yang, K;  Yan, W (reprint author), Chinese Acad Sci, Inst Met Res, Shenyang 110016, Liaoning, Peoples R China.;  Yan, W (reprint author), Chinese Acad Sci, Inst Met Res, Key Lab Nucl Mat & Safety Assessment, Shenyang 110016, Liaoning, Peoples R China.
收藏  |  浏览/下载:129/0  |  提交时间:2018/06/05
Bi Eutectic Alloy  Fe-9cr-1mo Steel  Stainless-steels  Resistance  Mechanism  Progress  
Lower-temperature aluminizing behaviors of a ferritic-martensitic steel processed by means of surface mechanical attrition treatment 期刊论文
Surface & Coatings Technology, 2014, 卷号: 258, 页码: 329-336
作者:  S.;  Wang Guo, Z. B.;  Wang, L. M.;  Lu, K.
收藏  |  浏览/下载:133/0  |  提交时间:2015/05/08
Nanostructured  Surface Mechanical Attrition Treatment (Smat)  Aluminization  Diffusion  Ferritic-martensitic Steel  Low-carbon Steel  Fe-al System  Reactive Diffusion  Nanostructured Fe  Coating Formation  Alloy-steels  Iron  Layer  Cr  Interdiffusion  
Magnetic domain structure and damping capacity of Fe-13Cr-2.5Mo alloy 期刊论文
Materials Science and Engineering B-Advanced Functional Solid-State Materials, 2010, 卷号: 171, 期号: 1-3, 页码: 40-44
作者:  X. F. Hu;  X. Y. Li;  B. Zhang;  L. J. Rong;  Y. Y. Li
Adobe PDF(1317Kb)  |  收藏  |  浏览/下载:130/0  |  提交时间:2012/04/13
Fe-cr-mo  Magnetic Domain  Damping  Bitter Technique  90 Degrees Domain  Wall  Internal Stress Distribution  Fe  Iron  Dependence  Mechanism  Crystals  Steels  
Effect of a small increase in the Ni content on the properties of a laser surface clad Fe-based alloy 期刊论文
Applied Surface Science, Applied Surface Science, 2007, 2007, 卷号: 253, 253, 期号: 9, 页码: 4420-4426, 4420-4426
作者:  X. Y. Yang;  X. A. Peng;  J. Chen;  F. H. Wang
收藏  |  浏览/下载:78/0  |  提交时间:2012/04/13
Fe-based Alloy  Fe-based Alloy  Laser Surface Cladding  Laser Surface Cladding  Microhardness  Microhardness  Electrochemical  Electrochemical  Corrosion  Corrosion  High Temperature Oxidation  High Temperature Oxidation  Stainless-steels  Stainless-steels  Solidification Mode  Solidification Mode  Tool Steels  Tool Steels  Cr  Cr  Coatings  Coatings  Behavior  Behavior  Stellite  Stellite  Microstructure  Microstructure  Susceptibility  Susceptibility  Parameters  Parameters  
The influence of Ni alloying on corrosion behaviour of low alloy steels under wet/dry cyclic conditions 期刊论文
Canadian Metallurgical Quarterly, 2007, 卷号: 46, 期号: 2, 页码: 195-205
作者:  X. Chen;  J. Dong;  E. Han;  W. Ke
收藏  |  浏览/下载:73/0  |  提交时间:2012/04/13
Industrial Environments  Weathering Steels  Carbon-steel  Alpha-feooh  Fe-ni  Rust  Iron  Cr  Atmospheres  Electrodes  
Corrosion behavior of three iron-based model alloys in reducing atmospheres containing HCl and H2S at 600 degrees C 期刊论文
Corrosion Science, 2007, 卷号: 49, 期号: 3, 页码: 1362-1377
作者:  T. J. Pan;  F. Gesmundo;  Y. Niu
收藏  |  浏览/下载:99/0  |  提交时间:2012/04/13
Fe-cr Alloys  Reducing Atmosphere  Oxidation  Hcl And H2s Effects  High-temperature Corrosion  Fe-cr Alloys  Municipal Incinerators  Hydrogen-chloride  Chromium-alloys  Oxidizing Atmospheres  Fireside  Corrosion  Commercial Steels  Containing Gas  Fired Boilers  
Air corrosion of Fe-15Cr-xAl alloys beneath KCl-ZnCl2 deposits at 773K 期刊论文
High Temperature Materials and Processes, 2006, 卷号: 25, 期号: 5-6, 页码: 255-260
作者:  T. J. Pan;  W. T. Wu;  C. L. Zeng;  Y. Niu
收藏  |  浏览/下载:97/0  |  提交时间:2012/04/14
Fe-cr-al  Al Effect  Kcl-zncl2  Chlorination  High-temperature Corrosion  Waste Incineration Environment  Stainless-steels  Cr  Fe  Oxidation  Zncl2-kcl  Behavior  Elements  Melt  
Effect of grain refinement on the resistance of 304 stainless steel to breakaway oxidation in wet air 期刊论文
Acta Materialia, 2005, 卷号: 53, 期号: 19, 页码: 5079-5088
作者:  X. Peng;  J. Yan;  Y. Zhou;  F. Wang
收藏  |  浏览/下载:77/0  |  提交时间:2012/04/14
Austenitic Steel  Dc Magnetron Sputtering  Grain Refining  Nanocrystalline  Oxidation  Oxide hydrOxide Evaporation  High-temperature Oxidation  Fe-cr Alloys  Water-vapor  Stainless-steels  Chromium Evaporation  Model Alloys  Thin-films  Diffusion  Behavior  
The corrosion of three commercial steels in reducing atmospheres containing HCl and H2S at 873 K 期刊论文
High Temperature Materials and Processes, 2005, 卷号: 24, 期号: 3, 页码: 193-203
作者:  T. J. Pan;  M. Al-Omary;  C. L. Zeng;  W. T. Wu;  Y. Niu
收藏  |  浏览/下载:101/0  |  提交时间:2012/04/14
Fe-cr Steels  Reducing Atmosphere  Corrosion  Hcl And H2s Effects  High-temperature Corrosion  Waste Incineration Environments  Iron-chromium-alloys  Hydrogen-chloride  Gas-mixtures  Oxidizing  Atmospheres  Oxygen Mixtures  Cr Alloys  Fe-cr  Oxidation  
Corrosion of iron and four commercial steels in a Cl-containing oxidizing atmosphere at 500 similar to 600 degrees C 期刊论文
Journal of Materials Science & Technology, 2004, 卷号: 20, 期号: 2, 页码: 213-216
作者:  K. Zhang;  Y. Niu;  C. L. Zeng;  W. T. Wu
收藏  |  浏览/下载:89/0  |  提交时间:2012/04/14
Commercial Steels  High Temperature  Chlorination  Waste Incineration  Fe-cr Alloys  High-temperature  Chloridation  Oxidation