IMR OpenIR

浏览/检索结果: 共8条,第1-8条 帮助

已选(0)清除 条数/页:   排序方式:
Corrosion Behavior of X52 Anti-H2S Pipeline Steel Exposed to High H2S Concentration Solutions at 90 degrees C 期刊论文
Journal of Materials Science & Technology, 2014, 卷号: 30, 期号: 5, 页码: 504-510
作者:  M. Liu;  J. Q. Wang;  W. Ke;  E. H. Han
收藏  |  浏览/下载:134/0  |  提交时间:2014/07/03
H2s Corrosion  X52 Anti-h2s Pipeline Steel  High Temperature  Iron  Sulfide  Hydrogen-sulfide  Iron  Morphology  Diagrams  
Corrosion behaviour of X52 pipeline steel in high H2S concentration solutions at temperatures ranging from 25 degrees C to 140 degrees C 期刊论文
Corrosion Engineering Science and Technology, 2013, 卷号: 48, 期号: 5, 页码: 380-387
作者:  M. Liu;  J. Wang;  W. Ke
收藏  |  浏览/下载:88/0  |  提交时间:2013/12/24
X52 Pipeline Steel  H2s Corrosion  High Temperature  Corrosion Products  Iron-sulfide Films  Hydrogen-sulfide  Solubility  Autoclaves  Morphology  Pressures  Diagrams  Media  Water  
Corrosion behavior of three iron-based model alloys in reducing atmospheres containing HCl and H2S at 600 degrees C 期刊论文
Corrosion Science, 2007, 卷号: 49, 期号: 3, 页码: 1362-1377
作者:  T. J. Pan;  F. Gesmundo;  Y. Niu
收藏  |  浏览/下载:98/0  |  提交时间:2012/04/13
Fe-cr Alloys  Reducing Atmosphere  Oxidation  Hcl And H2s Effects  High-temperature Corrosion  Fe-cr Alloys  Municipal Incinerators  Hydrogen-chloride  Chromium-alloys  Oxidizing Atmospheres  Fireside  Corrosion  Commercial Steels  Containing Gas  Fired Boilers  
Corrosion of three commercial steels under ZnCl2-KCl deposits in a reducing atmosphere containing HCl and H2S at 400-500 degrees C 期刊论文
Oxidation of Metals, Oxidation of Metals, 2007, 2007, 卷号: 67, 67, 期号: 1-2, 页码: 107-127, 107-127
作者:  T. J. Pan;  C. L. Zeng;  Y. Niu
收藏  |  浏览/下载:91/0  |  提交时间:2012/04/13
Steels  Steels  Chlorides  Chlorides  Reducing Atmosphere  Reducing Atmosphere  Corrosion  Corrosion  Hcl And H2s Effects  Hcl And H2s Effects  High-temperature Corrosion  High-temperature Corrosion  Alloys  Alloys  Oxidation  Oxidation  Mixtures  Mixtures  Nickel  Nickel  Iron  Iron  400-700-degrees-c  400-700-degrees-c  Environments  Environments  Chloridation  Chloridation  Chromium  Chromium  
湿H2S环境中金属材料腐蚀的研究 期刊论文
石油化工腐蚀与防护, 2007, 卷号: 24, 期号: 3, 页码: 22-25
作者:  张万贞
收藏  |  浏览/下载:10/0  |  提交时间:2024/01/08
metal material  H2 S corrosion  test standard  method and technique  金属材料  H2S腐蚀  试验标准  方法和手段  
The corrosion of three commercial steels in reducing atmospheres containing HCl and H2S at 873 K 期刊论文
High Temperature Materials and Processes, 2005, 卷号: 24, 期号: 3, 页码: 193-203
作者:  T. J. Pan;  M. Al-Omary;  C. L. Zeng;  W. T. Wu;  Y. Niu
收藏  |  浏览/下载:100/0  |  提交时间:2012/04/14
Fe-cr Steels  Reducing Atmosphere  Corrosion  Hcl And H2s Effects  High-temperature Corrosion  Waste Incineration Environments  Iron-chromium-alloys  Hydrogen-chloride  Gas-mixtures  Oxidizing  Atmospheres  Oxygen Mixtures  Cr Alloys  Fe-cr  Oxidation  
Study on the inhibition effect of polymer film of propargyl alcohol in Fe/H2SO4 send Fe/H2SO4+H2S systems 期刊论文
Acta Physico-Chimica Sinica, 1999, 卷号: 15, 期号: 8, 页码: 726-734
作者:  L. J. Yan;  Y. F. He;  H. C. Lin;  W. T. Wu
收藏  |  浏览/下载:59/0  |  提交时间:2012/04/14
Polymer Film Of Pa  H2s  Fe/h2so4  Inhibition Effect  Acetylenic Alcohols  Iron Corrosion  Adsorption  Acid  
CNDO/2 study on the action of hydrogen sulfide in the corrosion of iron in sulfuric acid solution 期刊论文
Acta Chimica Sinica, 1998, 卷号: 56, 期号: 11, 页码: 1055-1062
作者:  L. J. Yan;  L. Niu;  H. C. Lin;  W. T. Wu;  S. Z. Liu
收藏  |  浏览/下载:69/0  |  提交时间:2012/04/14
H2s  Iron  Corrosion Behavior  Cndo/2  Microscopic Mechanism  Polymers