IMR OpenIR

浏览/检索结果: 共25条,第1-10条 帮助

已选(0)清除 条数/页:   排序方式:
Exploration on the Stress-induced Internal Corrosion of NaCl-deposited GH4169 under humid intermediate temperature environments 期刊论文
CORROSION SCIENCE, 2023, 卷号: 224, 页码: 16
作者:  Wang, Wenquan;  Cui, Yu;  Liu, Rui;  Liu, Li;  Wang, Fuhui
收藏  |  浏览/下载:7/0  |  提交时间:2024/01/08
High -temperature corrosion  NaCl  Internal corrosion kinetics  Elastic stress  
Effect of NaCl-rich environment on internal corrosion for Ti60 alloy at 600 & DEG;C 期刊论文
CORROSION SCIENCE, 2023, 卷号: 220, 页码: 15
作者:  Chen, Wenzheng;  Li, Rui;  Liu, Li;  Liu, Rui;  Cui, Yu;  Chen, Zhiyong;  Wang, Qingjiang;  Wang, Fuhui
收藏  |  浏览/下载:7/0  |  提交时间:2024/01/07
Titanium  Alloy  High temperature corrosion  Internal oxidation  Ti60  

Internal microbiologically influenced corrosion of natural gas pipelines: A critical review

期刊论文

JOURNAL OF NATURAL GAS SCIENCE AND ENGINEERING, 2022, 卷号: 102, 页码: 14
作者:  Wei, Boxin;  Xu, Jin;  Sun, Cheng;  Cheng, Y. Frank
收藏  |  浏览/下载:109/0  |  提交时间:2022/07/14
Internal microbiologically influenced corrosion  Natural gas pipelines  Thin layers of electrolyte  Biofilm  Review  
Microstructure and stress corrosion cracking behavior of Alloy 690TT steam generator tubes with internal bulge defect 期刊论文
JOURNAL OF NUCLEAR MATERIALS, 2022, 卷号: 563, 页码: 14
作者:  Wu, Bin;  Ming, Hongliang;  Zhang, Zhiming;  Meng, Fanjiang;  He, Guangqing;  Wang, Jianqiu;  Han, En-Hou
收藏  |  浏览/下载:156/0  |  提交时间:2022/07/14
Alloy 690TT  Tube expansion  Internal bulge defect  Stress corrosion cracking  Intergranular corrosion  High temperature corrosion  

Revealing internal corrosion of GH4169 with stress coupled solid NaCl deposited in a humid environment of 600?

期刊论文

CORROSION SCIENCE, 2022, 卷号: 195, 页码: 13
作者:  Wang, Wenquan;  Cui, Yu;  Liu, Rui;  Liu, Li;  Wang, Fuhui
收藏  |  浏览/下载:90/0  |  提交时间:2022/07/01
High-temperature corrosion  Internal corrosion  Elastic stress  
Characteristics of Oxidation and Oxygen Penetration of Alloy 690 in 600 degrees C Aerated Supercritical Water 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2018, 卷号: 34, 期号: 3, 页码: 561-569
作者:  Zhong, XY;  Wu, XQ;  Han, EH;  Zhong, XY (reprint author), Chinese Acad Sci, Inst Met Res, Liaoning Key Lab Safety & Assessment Tech Nucl Ma, CAS Key Lab Nucl Mat & Safety Assessment, Shenyang 110016, Liaoning, Peoples R China.
收藏  |  浏览/下载:135/0  |  提交时间:2018/06/05
High-temperature Water  Nickel-base Alloys  Stress-corrosion Cracking  Surface Oxide-films  Intergranular Oxidation  Elevated-temperatures  Electron-microscopy  Internal Oxidation  Chromium Alloys  Behavior  
Internal Oxidation of Binary A-B Alloys by Two Oxidants: Double Internal Oxidation of B in the Presence of an External AX(m) Scale 期刊论文
Oxidation of Metals, 2015, 卷号: 83, 期号: 42067, 页码: 203-222
作者:  Q. Q.;  Liu Guo, L. L.;  Liu, S.;  Niu, Y.
收藏  |  浏览/下载:139/0  |  提交时间:2015/05/08
Internal Oxidation  Binary Alloys  Two Oxidants  Kinetics  Fe-si Alloys  High-temperature Corrosion  Degrees-c  Bcc Iron  Atmospheres  Solubility  Transition  Diffusion  Carbon  
Microstructure, mechanical, thermal, and oxidation properties of a Zr(2) Al(Si) (4)C(5)-SiC composite prepared by in situ reaction/hot-pressing 期刊论文
Journal of the European Ceramic Society, 2010, 卷号: 30, 期号: 11, 页码: 2147-2154
作者:  L. F. He;  F. Z. Li;  X. P. Lu;  Y. W. Bao;  Y. C. Zhou
Adobe PDF(1731Kb)  |  收藏  |  浏览/下载:103/0  |  提交时间:2012/04/13
Carbides  Microstructure  Mechanical Properties  Thermal Properties  Corrosion  High-temperature  Ti3si(Al)C-2/sic Composites  Fracture-toughness  Internal-friction  Silicon-carbide  c Ceramics  Zr2al3c4  Additives  Strength  Aluminum  
Accelerated corrosion of Fe-xCr-10Al alloys containing 0-20 at.% Cr induced by sulfur and chlorine in a reducing atmosphere at 600 degrees C 期刊论文
Oxidation of Metals, 2008, 卷号: 69, 期号: 1-2, 页码: 63-76
作者:  W. M. Lu;  T. J. Pan;  Y. Niu
Adobe PDF(496Kb)  |  收藏  |  浏览/下载:73/0  |  提交时间:2012/04/13
Fe-xcr-10al  Oxidation  Chlorine And Sulfur Effect  High-oxidant Pressures  Al-y Alloys  High-temperature Corrosion  Most-reactive Components  Internal Oxidation  Hydrogen-chloride  External Oxidation  Ternary Alloys  Iron  Oxygen  
Internal attack of Fe-xCr-10Al alloys induced by the presence of chlorine and sulfur in a reducing atmosphere at 973 K 期刊论文
Scripta Materialia, 2007, 卷号: 57, 期号: 2, 页码: 97-100
作者:  T. J. Pan;  Y. Niu
收藏  |  浏览/下载:77/0  |  提交时间:2012/04/13
Fe-xcr-10al Alloys  Internal Attack  Cl And s Effect  Most-reactive Components  High-oxidant Pressures  High-temperature  Corrosion Behavior  External Oxidation  Ternary Alloys  Iron  Chloridation  Transition  Chromium