IMR OpenIR

浏览/检索结果: 共12条,第1-10条 帮助

已选(0)清除 条数/页:   排序方式:
Electrochemical Behavior of Three 90Cu-10Ni Tubes from Different Manufacturers After Immersion in 3.5% NaCl Solution 期刊论文
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 卷号: 26, 期号: 4, 页码: 1701-1716
作者:  Ekerenam, Okpo O.;  Ma, Aili;  Zheng, Yugui;  Emori, Wilfred;  Ma, AL (reprint author), Chinese Acad Sci, Inst Met Res, Key Lab Nucl Mat & Safety Assessment, 62 Wencui Rd, Shenyang 110016, Peoples R China.
收藏  |  浏览/下载:106/0  |  提交时间:2017/08/17
Corrosion And Wear  Corrosion Product Film  Eis  Nonferrous Metals  Oxidation  Polarization Curves  Xps  
Degradation mechanism of micro-arc oxidation coatings on biodegradable Mg-Ca alloys: The influence of porosity 期刊论文
JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 卷号: 695, 页码: 2464-2476
作者:  Cui, Lan-Yue;  Zeng, Rong-Chang;  Guan, Shao-Kang;  Qi, Wei-Chen;  Zhang, Fen;  Li, Shuo-Qi;  Han, En-Hou;  Zeng, RC (reprint author), Shandong Univ Sci & Technol, Coll Mat Sci & Engn, Qingdao 266590, Peoples R China.
收藏  |  浏览/下载:103/0  |  提交时间:2017/08/17
Metals And Alloys  Thin Films  Corrosion  Oxidation  Sem  
Analysis of Surface Oxide Films Formed in Hydrogenated Primary Water on Alloy 690TT Samples With Different Surface States 期刊论文
Journal of Materials Science & Technology, 2014, 卷号: 30, 期号: 12, 页码: 1181-1192
作者:  Z. M.;  Wang Zhang, J. Q.;  Han, E. H.;  Ke, W.
收藏  |  浏览/下载:123/0  |  提交时间:2015/05/08
Alloy 690tt  Oxidation  Surface States  High Pressure And High  Temperature  High-temperature Water  Stress-corrosion Cracking  Nickel-based Alloys  Type-316 Stainless-steel  Mixed-conduction Model  X-ray Photoelectron  Fe-cr Alloys  Supercritical Water  288-degrees-c Water  Electrochemical-behavior  
Al、Ti、Ta对镍基定向高温合金组织与性能的影响 学位论文
, 北京: 中国科学院金属研究所, 2012
作者:  韩汾汾
收藏  |  浏览/下载:104/0  |  提交时间:2013/04/12
定向柱晶高温合金  持久拉伸性能  热裂  氧化  热腐蚀  Directionally Solidified Ni-base Superalloy  Creep And Tensile Property  Hot Tearing  Oxidation  Hot Corrosion  
Accelerated corrosion of Fe-xCr-10Al alloys containing 0-20 at.% Cr induced by sulfur and chlorine in a reducing atmosphere at 600 degrees C 期刊论文
Oxidation of Metals, 2008, 卷号: 69, 期号: 1-2, 页码: 63-76
作者:  W. M. Lu;  T. J. Pan;  Y. Niu
Adobe PDF(496Kb)  |  收藏  |  浏览/下载:74/0  |  提交时间:2012/04/13
Fe-xcr-10al  Oxidation  Chlorine And Sulfur Effect  High-oxidant Pressures  Al-y Alloys  High-temperature Corrosion  Most-reactive Components  Internal Oxidation  Hydrogen-chloride  External Oxidation  Ternary Alloys  Iron  Oxygen  
Internal attack of Fe-xCr-10Al alloys induced by the presence of chlorine and sulfur in a reducing atmosphere at 973 K 期刊论文
Scripta Materialia, 2007, 卷号: 57, 期号: 2, 页码: 97-100
作者:  T. J. Pan;  Y. Niu
收藏  |  浏览/下载:78/0  |  提交时间:2012/04/13
Fe-xcr-10al Alloys  Internal Attack  Cl And s Effect  Most-reactive Components  High-oxidant Pressures  High-temperature  Corrosion Behavior  External Oxidation  Ternary Alloys  Iron  Chloridation  Transition  Chromium  
Corrosion behavior of three iron-based model alloys in reducing atmospheres containing HCl and H2S at 600 degrees C 期刊论文
Corrosion Science, 2007, 卷号: 49, 期号: 3, 页码: 1362-1377
作者:  T. J. Pan;  F. Gesmundo;  Y. Niu
收藏  |  浏览/下载:95/0  |  提交时间:2012/04/13
Fe-cr Alloys  Reducing Atmosphere  Oxidation  Hcl And H2s Effects  High-temperature Corrosion  Fe-cr Alloys  Municipal Incinerators  Hydrogen-chloride  Chromium-alloys  Oxidizing Atmospheres  Fireside  Corrosion  Commercial Steels  Containing Gas  Fired Boilers  
Corrosion of three commercial steels under ZnCl2-KCl deposits in a reducing atmosphere containing HCl and H2S at 400-500 degrees C 期刊论文
Oxidation of Metals, Oxidation of Metals, 2007, 2007, 卷号: 67, 67, 期号: 1-2, 页码: 107-127, 107-127
作者:  T. J. Pan;  C. L. Zeng;  Y. Niu
收藏  |  浏览/下载:88/0  |  提交时间:2012/04/13
Steels  Steels  Chlorides  Chlorides  Reducing Atmosphere  Reducing Atmosphere  Corrosion  Corrosion  Hcl And H2s Effects  Hcl And H2s Effects  High-temperature Corrosion  High-temperature Corrosion  Alloys  Alloys  Oxidation  Oxidation  Mixtures  Mixtures  Nickel  Nickel  Iron  Iron  400-700-degrees-c  400-700-degrees-c  Environments  Environments  Chloridation  Chloridation  Chromium  Chromium  
Mechanical properties and oxidation behavior of a graded (Ti,Al)N coating deposited by arc-ion plating 期刊论文
Oxidation of Metals, 2006, 卷号: 65, 期号: 5-6, 页码: 307-327
作者:  C. J. Feng;  M. S. Li;  L. Xin;  S. L. Zhu;  F. H. Wang
收藏  |  浏览/下载:79/0  |  提交时间:2012/04/13
Arc-ion Plating (Aip)  Graded (Ti  Al)n Coating  Mechanical Properties  Oxidation And Corrosion  Chemical-vapor-deposition  Sputtered Tialn Films  High-speed Steel  Ti-al-n  Hard Coatings  Water-vapor  Thin-films  Chlorination  Corrosion  Nacl  
The oxidation behavior of TiAINb intermetallics with coatings at 800 C 期刊论文
Surface & Coatings Technology, 2005, 卷号: 197, 期号: 2-3, 页码: 322-326
作者:  Y. M. Xiong;  S. L. Zhu;  F. H. Wang
收藏  |  浏览/下载:67/0  |  提交时间:2012/04/14
Tialnb Intermetallics  Discontinuous And Cyclic Oxidation  Coatings  Tial-based Intermetallics  High-temperature Air  Titanium Aluminides  Nb  Addition  Ti60 Alloy  Resistance  Corrosion