Enhancing the high-temperature corrosion resistance of HVOF-sprayed NiCoCrAlY coating in marine environment by Pt modification and pre-oxidation 期刊论文
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2024, 卷号: 201, 页码: 222-235
作者:  Li, Y. Y.;  Jiang, Y. M.;  Zhang, C.;  Ji, H. Z.;  Li, S.;  Xu, N.;  Bao, Z. B.;  Zhu, S. L.;  Wang, F. H.
收藏  |  浏览/下载:2/0  |  提交时间:2025/04/27
High-temperature corrosion  HVOF-sprayed MCrAlY coating  Pt modification  Pre-oxidation  marine environment  
Effect of pre-oxidation on the corrosion behavior of Al-containing ODS steel in oxygen- saturated static LBE at 600 and 700°C 期刊论文
JOURNAL OF NUCLEAR MATERIALS, 2024, 卷号: 600, 页码: 14
作者:  Li, Xinle;  Bao, Feiyang;  Zhang, Jiarong;  Wang, Qitao;  Li, Yaozhi;  Yin, Mengjie;  Yan, Wei;  Li, Yanfen
收藏  |  浏览/下载:3/0  |  提交时间:2025/04/27
lead-bismuth eutectic (LBE)  Oxide dispersion strengthened steel (ODS)  Pre-oxidation  Corrosion  
Effect of pre-oxidation on the corrosion behavior of Al-containing ODS steel in oxygen- saturated static LBE at 600 and 700°C 期刊论文
JOURNAL OF NUCLEAR MATERIALS, 2024, 卷号: 600, 页码: 14
作者:  Li, Xinle;  Bao, Feiyang;  Zhang, Jiarong;  Wang, Qitao;  Li, Yaozhi;  Yin, Mengjie;  Yan, Wei;  Li, Yanfen
收藏  |  浏览/下载:3/0  |  提交时间:2025/04/27
lead-bismuth eutectic (LBE)  Oxide dispersion strengthened steel (ODS)  Pre-oxidation  Corrosion  
Corrosion Behavior of Pre-oxidized GH4169 Alloy with Solid NaCl Deposited in a Wet Oxygen Flow at 600 °C 期刊论文
ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2024, 页码: 16
作者:  Zhang, Weidong;  Cui, Yu;  Liu, Li;  Wang, Wenquan;  Chen, Wenzheng;  Li, Rui;  Wang, Fuhui
收藏  |  浏览/下载:2/0  |  提交时间:2025/04/27
Pre-oxidation  Solid NaCl  Wet O-2  Electrochemical corrosion  
High-temperature corrosion behaviour of Pt-modified aluminide coating with solid NaCl deposit in O-2+10 vol% H2O and the influence of pre-oxidation treatment 期刊论文
CORROSION SCIENCE, 2022, 卷号: 204, 页码: 12
作者:  Li, Y. Y.;  Huang, D.;  Zhang, C. Y.;  Li, S.;  Bao, Z. B.;  Zhu, S. L.;  Wang, F. H.
收藏  |  浏览/下载:118/0  |  提交时间:2022/09/16
Pt-modified aluminide coating  Corrosion performance  Chlorination  Water vapour  Pre-oxidation  
Effects of pellet surface roughness and pre-oxidation temperature on CMAS corrosion behavior of Ti2AlC 期刊论文
JOURNAL OF ADVANCED CERAMICS, 2022, 卷号: 11, 期号: 6, 页码: 945-960
作者:  Guo, Lei;  Li, Guang;  Wu, Jing;  Wang, Xiaohui
收藏  |  浏览/下载:106/0  |  提交时间:2022/07/14
thermal barrier coatings (TBCs)  Ti2AlC  surface roughness  pre-oxidation temperature  calcium-magnesium-alumina-silicate (CMAS) corrosion  thermal cycling  
Effect of pre-oxidation on the failure mechanisms of EB-PVD thermal barrier coatings with (Ni,Pt)Al bond coats 期刊论文
CORROSION SCIENCE, 2021, 卷号: 193, 页码: 11
作者:  Li, S.;  Xu, M. M.;  Zhang, C. Y.;  Bao, Z. B.;  Yang, Y. F.;  Zhu, S. L.;  Wang, F. H.
收藏  |  浏览/下载:137/0  |  提交时间:2021/11/22
Thermal barrier coatings  Platinum  Pre-oxidation  Intermixed zone  Failure mechanism  
High temperature oxidation behavior of Ni-based superalloy Nimonic95 and the effect of pre-oxidation treatment 期刊论文
VACUUM, 2021, 卷号: 194, 页码: 11
作者:  Li, Danhong;  Chen, Junxiu;  Etim, Iniobong P.;  Liu, Ya;  Wu, Changjun;  Wang, Jianhua;  Su, Xuping
收藏  |  浏览/下载:131/0  |  提交时间:2021/11/22
Ni-based superalloy  Oxidation behavior  High-temperature pre-oxidation  
Oxide Scale Formation on Ultrafine-Grained Ferritic-Martensitic Steel During Pre-Oxidation and Its Effect on the Corrosion Performance in Stagnant Liquid Pb-Bi Eutectic 期刊论文
ACTA METALLURGICA SINICA, 2021, 卷号: 57, 期号: 8, 页码: 989-999
作者:  Chen Shenghu;  Rong Lijian
收藏  |  浏览/下载:173/0  |  提交时间:2021/10/15
ultrafine-grained ferritic-martensitic steel  cold rotary-swaging deformation  pre-oxidation  Pb-Bi corrosion  diffusion  
Activation treatment effects on characteristics of BeO layer and secondary electron emission properties of an activated Cu-Be alloy 期刊论文
APPLIED SURFACE SCIENCE, 2015, 卷号: 355, 页码: 19-25
作者:  Wang, Bin;  Wu, Erdong;  Wang, Yongli;  Xiong, Liangyin;  Liu, Shi;  sliu@imr.ac.cn
收藏  |  浏览/下载:129/0  |  提交时间:2016/04/21
Thickness And Composition Distribution Of Beo Layer  Oxidation Duration  Oxidation Temperature  Pre-heat Treatment  Oxygen Pressure